MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Polyplastic Compounds Armlen® PP MF 20-18IM (Natural) Polypropylene, Impact Modified
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene, Impact Modified; Molded/Extruded

Material Notes: Impact modified polypropylene composite material for interior and exterior trims, UV- resistant.

Information provided by Polyplastic Compounds

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.00 - 1.05 g/cc0.0361 - 0.0379 lb/in³ISO 1183
Melt Flow 12 - 19 g/10 min
@Load 2.16 kg,
Temperature 230 °C
12 - 19 g/10 min
@Load 4.76 lb,
Temperature 446 °F
ISO 1133
Ash 13 - 18 %13 - 18 %ISO 3451-1
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield >= 17.0 MPa>= 2470 psiISO 527-2
Tensile Modulus >= 1.45 GPa>= 210 ksiISO 527-2
Flexural Modulus >= 1.60 GPa>= 232 ksiISO 178
Izod Impact, Notched (ISO)  >= 3.00 kJ/m²
@Temperature -40.0 °C
>= 1.43 ft-lb/in²
@Temperature -40.0 °F
ISO 180/A
 >= 20.0 kJ/m²
@Temperature 23.0 °C
>= 9.52 ft-lb/in²
@Temperature 73.4 °F
ISO 180/A
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) >= 93.0 °C>= 199 °FISO 75B
Deflection Temperature at 1.8 MPa (264 psi) >= 50.0 °C>= 122 °FISO 75A
Shrinkage 0.90 - 1.2 %0.90 - 1.2 %ISO 294-4
 
Processing PropertiesMetricEnglishComments
Melt Temperature 220 - 230 °C428 - 446 °F
Mold Temperature 60.0 °C140 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PPOLPLC090 / 307162

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.