MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

TIMET TIMETAL® 3-2.5-0.05Pd Titanium Alloy
Categories: Metal; Nonferrous Metal; Titanium Alloy; Alpha/Near Alpha Titanium Alloy

Material Notes: Cold Workable Medium Strength Alloy. Palladium is added to this grade to enhance its corrosion behavior. Property data below is typical of TIMETAL® 3-2.5 Titanium Alloy.

Data provided by TIMET.

Key Words: Titanium 3-2.5
Vendors: Visit metalmen for your metals needs. Products include special chemistry, tight tolerances, custom tempers, odd dimensions/forms, and small quantities. Phone 1-800-767-9494.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 4.51 g/cc0.163 lb/in³Typical
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate 650 MPa94300 psiTypical
Tensile Strength, Yield 550 MPa
@Strain 0.2 %
79800 psi
@Strain 0.2 %
Typical
Elongation at Break 15 %15 %Typical
Modulus of Elasticity 105 - 120 GPa15200 - 17400 ksiTypical
Poissons Ratio 0.300.30
Shear Modulus 43.0 - 45.0 GPa6240 - 6530 ksi
Bend Radius, Minimum 2.5 t2.5 tTypical; on 0.078 in (2 mm) sheet
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.000127 ohm-cm0.000127 ohm-cm
 
Thermal PropertiesMetricEnglishComments
CTE, linear 9.61 µm/m-°C
@Temperature 20.0 - 95.0 °C
5.34 µin/in-°F
@Temperature 68.0 - 203 °F
Thermal Conductivity 8.30 W/m-K
@Temperature 20.0 - 95.0 °C
57.6 BTU-in/hr-ft²-°F
@Temperature 68.0 - 203 °F
Melting Point <= 1700 °C<= 3090 °F
Liquidus 1700 °C3090 °F
Beta Transus 935 °C1720 °F
 
Component Elements PropertiesMetricEnglishComments
Aluminum, Al 2.5 - 3.5 %2.5 - 3.5 %
Carbon, C <= 0.080 %<= 0.080 %
Hydrogen, H <= 0.015 %<= 0.015 %
Iron, Fe <= 0.25 %<= 0.25 %
Nitrogen, N <= 0.030 %<= 0.030 %
Other, each <= 0.10 %<= 0.10 %
Other, total <= 0.40 %<= 0.40 %
Oxygen, O <= 0.15 %<= 0.15 %
Palladium, Pd 0.040 - 0.080 %0.040 - 0.080 %
Titanium, Ti 92.5 - 95.5 %92.5 - 95.5 %Calculated as remainder
Vanadium, V 2.0 - 3.0 %2.0 - 3.0 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Titanium Ti-8Al-1Mo-1V (Ti-8-1-1), Beta Solution Treated
TIMET TIMETAL® 5111 Titanium Alloy (Ti-5Al-1Sn-1Zr-1V-0.8Mo; ASTM Grade 32)
Titanium Ti-6Al-2Sn-4Zr-2Mo-0.1Si; Duplex Annealed
ATI Allvac® 6-2-4-2 Titanium Alloy, Heat Treatment: 982°C (1800°F) + Age
Overview of materials for Alpha/Near Alpha Titanium Alloy

NTIME325P / 19298

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.