SABIC® PPcompound 9120 is an elastomer-modified mineral filled Polypropylene with excellent impact and stiffness ratio. Typical material applications are esthetical automotive interior parts. It has a very high scratch resistance, no stickiness and a high flow.
SABIC® PPcompound 9120 is a designated automotive grade.
IMDS ID: 115845433Information provided by SABIC |