MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Carmel Olefins Capilene® U 77 A Polypropylene Homopolymer
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene, Molded

Material Notes: Description: CAPILENE® U 77 A is a high melt flow rate homopolymer for injection molding of products with long flow length. It is specially formulated with antistatic and nucleating additives, allowing fast cycle due to high de-molding temperature and reduced cooling time. It exhibits high stiffness combined with high flowability and good contact clarity.

Applications: CAPILENE® U 77 A is designed for multi-cavity injection molding, thin walled packaging items, products with long flow length, household articles and toys. In comparison to CAPILENE® U 77 AV it offers a better choice for food packaging containers.

Information provided by Carmel Olefins.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Melt Flow 35 g/10 min
@Load 2.16 kg,
Temperature 230 °C
35 g/10 min
@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 36.0 MPa5220 psi50 mm/min; ASTM D638
Elongation at Yield 11 %11 %50 mm/min; ASTM D638
Flexural Modulus 1.80 GPa261 ksiASTM D790
Izod Impact, Notched 0.250 J/cm0.468 ft-lb/inASTM D256
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 110 °C230 °FASTM D648
Vicat Softening Point 155 °C
@Load 1.02 kg
311 °F
@Load 2.25 lb
ASTM D1525

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Carmel Olefins Capilene® U 77 AV Polypropylene Homopolymer
Polyram RamOfin RPPC711 Polypropylene, UV Stabilized
Braskem H 504 XP Bioriented Film Polypropylene
Birch Plastics RPP1215 Recycled Polypropylene
Buckeye Polymers BP RPPC 1813 C BLK Polypropylene, Calcium Filled

PCARM975 / 131150

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.