MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

ExxonMobil Escorene® LL-3002 LLDPE/Hexene Premium Cast Stretch Film Resin, 1.2 mil Film  (discontinued **)
Categories: Polymer; Film; Thermoplastic; Polyethylene (PE); Linear Low Density (LLDPE); Linear Low Density Polyethylene (LLDPE), Film Grade; LLDPE/Hexene, Film Grade

Material Notes: Data provided by the manufacturer, Exxon Chemical.

A hexene copolymer LLDPE cast film resin. Films made from LL-3002 have outstanding tensile properties as well as stiffness and toughness. These superior properties combined with the resin's good drawdown make LL-3002 a very versatile packaging film resin.

Applications: Stretch wrap film; Premium packaging film. Data for film properties below based on 1.2 mil film.

Key Words: Linear Low Density Polyethylene; Exxon Chemical Company
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.917 g/cc0.0331 lb/in³Exxon Method
Thickness 30.5 microns1.20 mil
Melt Flow 2.0 g/10 min2.0 g/10 minExxon Method
 
Mechanical PropertiesMetricEnglishComments
Film Tensile Strength at Yield, MD 9.70 MPa1410 psiASTM D882
Film Tensile Strength at Yield, TD 10.3 MPa1490 psiASTM D882
Film Elongation at Break, MD 650 %650 %ASTM D882
Film Elongation at Break, TD 750 %750 %ASTM D882
Secant Modulus, MD 0.207 GPa30.0 ksiASTM D882
Secant Modulus, TD 0.262 GPa38.0 ksiASTM D882
Elmendorf Tear Strength MD 250 g250 gASTM D1922
Elmendorf Tear Strength TD 680 g680 gASTM D1922
Elmendorf Tear Strength, MD 8.19 g/micron208 g/milASTM D1922
Elmendorf Tear Strength, TD 22.3 g/micron567 g/milASTM D1922
Dart Drop 3.94 g/micron100 g/milF50; ASTM D1709
Dart Drop Test 120 g0.265 lbF50; ASTM D-1709
Film Tensile Strength at Break, MD 52.1 MPa7560 psiASTM D882
Film Tensile Strength at Break, TD 37.9 MPa5500 psiASTM D882
 
Thermal PropertiesMetricEnglishComments
Melting Point 124 °C255 °FExxon Method
 
Optical PropertiesMetricEnglishComments
Haze 12 %12 %ASTM D1003
Gloss 53 %53 %45°, ASTM D-2457

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PEXCGO / 37972

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.