MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Henkel Hysol PL 7000 Film Adhesive
Categories: Polymer; Adhesive; Film; Thermoset; Epoxy; Epoxy Adhesive

Material Notes: Epoxy film adhesive formulated to provide excellent performance properties in composite bonding, and has excellent results on composite surfaces that have been exposed to bond shop environments and may have absorbed moisture. Excellent fracture toughness (G1C) over composite surfaces exhibiting cohesive failure patterns, indicating superior adhesion characteristics. Qualified at Boeing.

Application: Composite Surfacing

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Storage Temperature -18.0 °C-0.400 °F
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 7.40 MPa1070 psiFlatwise
Adhesive Bond Strength  9.00 MPa
@Temperature 132 °C
1310 psi
@Temperature 270 °F
Lap Shear
 26.2 MPa
@Temperature -55.0 °C
3800 psi
@Temperature -67.0 °F
Lap Shear
 31.0 MPa
@Temperature 25.0 °C
4500 psi
@Temperature 77.0 °F
Lap Shear
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 149 °C300 °F
Glass Transition Temp, Tg 62.5 °C145 °Fdry
 
Processing PropertiesMetricEnglishComments
Cure Time  60.0 - 120 min
@Temperature 177 °C
1.00 - 2.00 hour
@Temperature 351 °F
 90.0 - 120 min
@Temperature 121 °C
1.50 - 2.00 hour
@Temperature 250 °F
 
Descriptive Properties
Out-Time (days)30at 25°C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
3M Scotch-Weld™ 2216 B/A Gray Epoxy Adhesive
Henkel Loctite® Durabond® E-30CL Epoxy Adhesive
Momentive Performance Materials RTV142 White, Low Volatile, One Component Silicone Sealant
Barlog Plastics KEBAPEAK XS1700 PEEK, unreinforced
Barlog Plastics KEBAPEAK XF1730 PEEK, 30% glass fiber reinforced

PHENK844 / 146849

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.