MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Amity Thermosets ATS 766 Phenolic Molding Chopped cotton fabric Filler, Compression Molded
Categories: Polymer; Thermoset; Filled/Reinforced Thermoset; Phenolic

Material Notes:

Characteristics:

  • High impact strength
  • Glossy surface
  • Low shrinkage
  • Good sliding properties
  • Color-Brown
  • Medium flow
  • Applications:

  • Cog wheels
  • Castor wheels
  • Bush bearings
  • Pulleys
  • Welding rod handles
  • Textile bobbins etc.
  • Information provided by Amity Thermosets Limited

    Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
     
    Physical PropertiesMetricEnglishComments
    Density 1.38 - 1.46 g/cc0.0499 - 0.0527 lb/in³Molding; IS 867-1963
    Water Absorption 0.60 - 1.0 %0.60 - 1.0 %IS 13411-1993
    Linear Mold Shrinkage 0.0032 - 0.0049 cm/cm0.0032 - 0.0049 in/inIS 13411-1992
     
    Mechanical PropertiesMetricEnglishComments
    Tensile Strength at Break >= 35.0 MPa>= 5080 psi5 mm/min.; IS 867-1963
    Shear Strength >= 56.0 MPa>= 8120 psi2mm/min.; IS 867-1963
    Izod Impact, Notched >= 1.55 J/cm>= 2.90 ft-lb/inIS 13411-1992
     
    Processing PropertiesMetricEnglishComments
    Mold Temperature 160 - 170 °C320 - 338 °F
    Injection Pressure 15.68 - 34.3 MPa2274 - 4970 psiMold Pressure
    Cure Time 0.333 - 0.500 min0.00556 - 0.00833 hourper mm
    Shelf Life 12.0 Month12.0 Month

    Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

    Users viewing this material also viewed the following:
    Sumitomo Bakelite North America CF 9040A Carbon Fiber Reinforced Phenolic
    Rogers Arlon 0.008" (0.2032 mm) Flexible Heater Silicone with Fiberglass Substrate (44571R008)
    Covestro Bayflex® 180 Polyurethane Elastomeric RIM, 20% Mica Filled, MDI-based 2-Component Liquid System
    Covestro Baydur® SFR-243 Polyurethane Composite RRIM Foam, 15% Milled Glass Filled, MDI-based 2-Component Liquid System
    Cosmic Plastics D72 Short Glass Fiber Filled Ortho Diallyl Phthalate Molding Compound

    PAMITY02 / 24030

    Visit Zeus Inc. for PEEK Tubing

    Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

    The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.