MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
ExxonMobil Escorene® LD 761.36 Molding, extrusion and compounding resin
Categories: Polymer; Thermoplastic; Ethylene Vinyl Acetate; Ethylene Vinyl Acetate Copolymer (EVA), Extrusion/Coating Grade

Material Notes: Escorene Ultra LD 761.36 is a 26.7% vinyl acetate copolymer excellent flexibility and low temperature toughness. LD 761.36 has high filler acceptance.

Availability: Latin America, North America and South America

Additive:

  • Antiblock: No
  • Slip: No
  • Thermal Stabilizer: Yes
Applications:
  • Compounding
  • Masterbatch Base Resin
  • Profile Extrusion
  • Tube Extrusion

Information provided by ExxonMobil Chemical

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.951 g/ccExxonMobil Method
Vinyl Acetate Content 26.7 %ExxonMobil Method
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 7615s; ASTM D2240
Hardness, Shore D 2715s; ASTM D2240
Tensile Strength at Break 1200 psiASTM D638
Elongation at Break >= 800 %ASTM D638
Flexural Modulus, 1% Secant 4100 psiASTM D790
Instrumented Impact Total Energy 14.0 ft-lb
@Temperature 23.0 °C
ASTM D3763
 22.0 ft-lb
@Temperature -40.0 °C
ASTM D3763
 
Thermal PropertiesOriginal ValueComments
Melting Point 163 °FPeak Melting Temperature; ExxonMobil Method
Vicat Softening Point 115 °FASTM D1525
 
Descriptive Properties
FeaturesThermal Stabilizer

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Celanese Ateva® 1081G Medical Grade EVA
Dow Elvax® 3124 Ethylene-Vinyl Acetate Copolymer Resin for Extrusion Coating
Dow Elvax® 440 Ethylene Vinyl Acetate
Dow Bynel® 3861 Anhydride-Modified Ethylene Vinyl Acetate Adhesive Resin
Dow Bynel® 1123 Modified EVA Adhesive Resin

PEXB153 / 37458

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.