MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

Chase Electronic Coatings HumiSeal® 1B59LU Rubber Conformal Coating
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE)

Material Notes: HumiSeal® 1B59LU is an air drying, single component, synthetic rubber conformal coating. The unique chemistry, of HumiSeal® 1B59LU imparts extremely low moisture vapor permeability and improved heat resistance. The coating demonstrates excellent flexibility, low stress on components, fluoresces under UV for ease of inspection and is easily repaired. The coating is in full compliance with the RoHS Directive 2011/65/EC and meets the requirements of IPC-CC-830.

Information provided by Chase Electronic Coatings.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.790 g/cc0.0285 lb/in³ASTM D1475
Solids Content 18.5 %18.5 %By weight, ± 1.5%; Fed-Std-141, Meth. 4044
Volatile Organic Compounds (VOC) Content 648 g/l648 g/l
Water Vapor Transmission 26.0 g/m²/day
@Temperature 40.0 °C
1.67 g/100 in²/day
@Temperature 104 °F
90% R.H
Viscosity 140 - 280 cP140 - 280 cPFed-Std-141, Meth. 4287. Part A
Thickness 25.0 - 75.0 microns0.984 - 2.95 milRecommended coating
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 8.50e+15 ohm-cm8.50e+15 ohm-cm
Surface Resistance 3.10e+9 ohm
@Temperature 85.0 °C
3.10e+9 ohm
@Temperature 185 °F
85% RH, 50V
Surface Resistivity per Square 2.60e+15 ohm2.60e+15 ohm
Insulation Resistance 1.80e+10 ohm1.80e+10 ohmMoisture; MIL-I-46058C
 8.40e+12 ohm8.40e+12 ohmMIL-I-46058C
Dielectric Constant 1.9
@Frequency 1e+6 Hz,
Temperature 23.0 °C
1.9
@Frequency 1e+6 Hz,
Temperature 73.4 °F
Dielectric Strength 85.0 kV/mm2160 kV/inJIS C2110.8.2.
Dissipation Factor 0.0040
@Frequency 1e+6 Hz,
Temperature 23.0 °C
0.0040
@Frequency 1e+6 Hz,
Temperature 73.4 °F
 
Thermal PropertiesMetricEnglishComments
CTE, linear  18.5 µm/m-°C
@Temperature <=-49.6 °C
10.3 µin/in-°F
@Temperature <=-57.3 °F
Below Tg; TMA
 130 µm/m-°C
@Temperature >=-49.6 °C
72.2 µin/in-°F
@Temperature >=-57.3 °F
Above Tg; TMA
Maximum Service Temperature, Air 150 °C302 °F
Minimum Service Temperature, Air -65.0 °C-85.0 °F
Glass Transition Temp, Tg -49.6 °C-57.3 °FDSC
 
Processing PropertiesMetricEnglishComments
Cure Time  300 min
@Temperature 76.0 °C
5.00 hour
@Temperature 169 °F
Option
 1440 min
@Temperature 23.0 °C
24.0 hour
@Temperature 73.4 °F
 10100 min
@Temperature 23.0 °C
168 hour
@Temperature 73.4 °F
Optimum Properties
Tack-Free Time 6.00 - 10.2 min0.100 - 0.170 hourFed-Std-141, Meth. 4061
Shelf Life 6.00 Month
@Temperature 23.0 °C
6.00 Month
@Temperature 73.4 °F
DOM
 
Descriptive Properties
Dielectric Withstand>1500 Vper MIL_I_46058C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PCHAS931 / 239792

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.