MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Austin Novel Materials Innonen® B90A Polyester-based TPU Elastomer
Categories: Polymer; Thermoplastic; Polyurethane, TP; Thermoplastic Polyurethane, Elastomer, Polyester Grade

Material Notes: This series of TPUs features good abrasion resistance, tensile strength, and oil resistance.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.17 - 1.21 g/ccISO 1183
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 87 - 93ISO 7619
Tensile Strength >= 40.0 MPaISO 37
Elongation at Break >= 480 %ISO 37
100% Modulus >= 8.00 MPa
@Strain 100 %
ISO 37
300% Modulus >= 14.0 MPa
@Strain 300 %
ISO 37
Tear Strength >= 105 kN/mISO 34
Abrasion <= 60mm3; ISO 4649
Compression Set <= 45 %
@Temperature 70.0 °C
ISO 815

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
TSE Industries EcoWIND® 100 Polyurethane Resin Filament Winding
Coastal Enterprises Plus™ PBHT-15 High Density Urethane Foam
Austin Novel Materials Innonen® H55A Polyester-based TPU Elastomer
Alliance Polymers Zythane™ 3045D Thermoplastic Polyurethane Elastomer

PDAWNE071 / 233362

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.