MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

CRP  Windform

(Viewing data as-entered. Click here to return)
3D Systems DuraForm® HST Fiber Filled Nylon for SLS Systems
Categories: Polymer; 3D Printing/Additive Manufacturing Polymer; Thermoplastic; Nylon (Polyamide PA)

Material Notes: Fiber filled nylon with anisotropic mechanical properties akin to fiber-filled, injection molded materials, allowing realistic testing of functional prototypes. It is ideal for functional prototypes and end-use parts that require high stiffness and/or elevated thermal resistance.

Applications include UAV structural components, housings and enclosures, impellers, connectors, and consumer sporting goods.

Information provided by 3D Systems.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.20 g/ccASTM D792
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 75ASTM D2240
Tensile Strength, Ultimate 48.0 - 51.0 MPaASTM D638
Elongation at Break 4.5 %ASTM D638
Tensile Modulus 5475 - 5725 MPaASTM D638
Flexural Strength 83.0 - 89.0 MPaASTM D790
Flexural Modulus 4400 - 4550 MPaASTM D790
Izod Impact, Notched 37.4 J/m
@Temperature 23.0 °C
ASTM D256
Izod Impact, Unnotched 3.10 J/cm
@Temperature 23.0 °C
ASTM D256
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 184 °CASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 179 °CASTM D648
Flammability, UL94 HB
@Thickness 3.00 mm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
LG Chemical LUMID GP2309A(W) PA6+GF30%, General Purpose
CRP Technology Windform® RL Thermoplastic Elastomer for SLS
BASF Ultramid® 8202 PA6 (Dry)
Celanese Celstran® TPU-GF30-01-US TPU, 30% Glass Reinforced
Huntsman IROGRAN® A 92 P 4637 TPU-Polyether

PAPPR120f / 191508

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.