MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

Oxford Polymers C-Acetal 10MF-900 BK Acetal
Categories: Polymer; Thermoplastic; Acetal (Polyoxymethylene, POM); Acetal Homopolymer, Unreinforced

Material Notes: Product Description: Acetal Injection Molding Grade, 10 melt flow

Processing and Delivery Form: Pellets and Injection Molding

Special Characteristics: Pre-colored black

Information provided by Oxford Polymers

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.41 g/cc0.0509 lb/in³ASTM D792
Water Absorption at Saturation 0.20 %0.20 %ASTM D570
Linear Mold Shrinkage, Flow 0.022 cm/cm
@Thickness 3.17 mm
0.022 in/in
@Thickness 0.125 in
ASTM D955
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 53.8 MPa7800 psiASTM D638
Elongation at Break 10 %10 %ASTM D638
Flexural Strength 68.9 MPa10000 psiASTM D790
Flexural Modulus 3.14 GPa455 ksiASTM D790
Izod Impact, Notched 0.427 J/cm
@Thickness 3.17 mm
0.800 ft-lb/in
@Thickness 0.125 in
ASTM D256
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) 107 °C225 °FUnannealed; ASTM D648
 
Processing PropertiesMetricEnglishComments
Rear Barrel Temperature 177 - 193 °C350 - 380 °F
Middle Barrel Temperature 182 - 199 °C360 - 390 °F
Front Barrel Temperature 188 - 204 °C370 - 400 °F
Nozzle Temperature 188 - 204 °C370 - 400 °F
Melt Temperature 182 - 218 °C360 - 425 °F
Mold Temperature 79.4 - 107 °C175 - 225 °F
Drying Temperature <= 93.3 °C<= 200 °F
Dry Time 2.00 - 3.00 hour2.00 - 3.00 hour

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

POXF003 / 178433

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.