MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Zircar Ceramics ECO-20AA Alumina Insulation
Categories: Ceramic; Oxide; Aluminum Oxide

Material Notes: ECO-20AA is most commonly utilized as hotface insulation in furnaces with hydrogen rich atmospheres such as bright annealing furnaces.

Information provided by Zircar Ceramics.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.310 g/cc
 
Mechanical PropertiesOriginal ValueComments
Flexural Strength 0.310 MPaParallel to thickness
Compressive Yield Strength 0.110 MPaat 10% Compression, Parallel to thickness
 
Thermal PropertiesOriginal ValueComments
Specific Heat Capacity 0.250 BTU/lb-°F
Thermal Conductivity 0.0900 W/m-K
@Temperature 400 °C
parallel to thickness; ASTM C177-76
 0.210 W/m-K
@Temperature 1200 °C
Parallel to Thickness; ASTM C177-76
Maximum Service Temperature, Air 1600 °C
Shrinkage 1.5 %
@Temperature 1650 °C,
Time 3600 sec
Perpendicular to Thickness
 4.0 %
@Treatment Temp. 1500 °C,
Time 14400 sec
Sag/Distortion, 1in. x 1in. beam on 5in. Span
 
Component Elements PropertiesOriginal ValueComments
Al2O3 98 %
SiO2 2.0 %
 
Descriptive Properties
ColorWhite

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Zircar Ceramics AL-25/1700 Alumina Insulation
Zircar Ceramics AL-30 Alumina Insulation
Zircar Ceramics AL-30AA Alumina Insulation
Zircar Ceramics AL-30AAH Alumina Insulation
Zircar Ceramics SALI Alumina Insulation

CZIR050 / 2858

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.