MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Covestro Bayhydrol® UV 2689/1 Polyurethane Coating
Categories: Polymer; Thermoplastic; Adhesives, Sealants, and Coatings; Thermoset; Polyurethane, TS

Material Notes: Bayhydrol UV 2689/1 is an anionic, UV-curable polyurethane dispersion. Bayhydrol UV 2689/1 is used in the formulation of industrial waterborne UV clear and pigmented coatings. Main applications are plastic coatings (e.g mobile phones) and wood coatings. Before UV curing the surface of dried films is soft and slightly tacky. After UV-cure the coatings are hard with high chemical and mechanical resistance. The product is suitable to achieve high gloss coatings.

Properties / Applications: Bayhydrol UV 2689/1 is used for the formulation of waterborne UV coatings, in particular for plastic applications. The addition of 1.0 to 2.5 weight % photoinitiator relative to binder has proven effective for initiation. We achieved good results with Irgacure® 500, Irgacure® 127, Irgacure® 819 DW (Ciba) and Esacure® KIP 100F (Lamberti). Viscosity is set by the addition of polyurethane thickeners for clear coats or acrylic thickeners for metallic effect coatings. As the dispersion has a relatively high surface tension the formulation should always contain a wetting agent, e.g. BYK® 348 (BYK) to avoid surface defects. Matting agents and additives can be dispersed directly into the formulation using a dissolver. Bayhydrol® UV 2689/1 can be easily matted using common matting agents. The formulation of metallic effect coatings using suitable metallic pigments is also possible. The product can also be combined with Bayhydur® or other hardeners to formulate ”dual cure ” waterborne UV coatings. After evaporation of the water and before UV-cure, the coatings are soft and slightly tacky. Water-free coatings can be cured with suitable UV-curing equipment at a line speed of typically 5 to 10 m/min per 80 W/cm lamp. To achieve the best film properties the coating temperature should be higher than 60°C when entering the UV zone. Care has to be taken if temperature sensitive materials are cured in this way. During UV curing a further temperature increase of 20 to 60°C is possible depending on conditions. UV curing yields surfaces with high hardness, very good mechanical strength and excellent chemical resistance especially against cosmetics. As with any product, use of Bayhydrol UV 2689/1 in a given application must be tested (including but not limited to field testing) in advance by the user to determine suitability.

Information provided by Covestro

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Volatiles 56 - 60 %1g/1h/125 °C/convection oven
pH 7.0 - 8.5
 
Descriptive Properties
Flow time15-50s4 mm cup
Pendulum hardness190s

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PCOVEST0185 / 201968

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.