MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Phillips 66 Syndustrial® ISO Grade 22/32 Turbine Oil
Categories: Fluid; Lubricant

Material Notes: Syndustrial Turbine Oil is a premium quality synthetic lubricant developed to meet the severe lubrication requirements of aero-derivative stationary and marine gas turbines. Syndustrial Turbine Oil is formulated with synthetic polyol ester (POE) base oils and select ashless additives to provide outstanding performance and protection in gas turbines. It has outstanding oxidation resistance and thermal stability at high temperatures to minimize deposit formation and provide long service life. It has high load-carrying capacity and excellent affinity for metal surfaces to protect against wear. It has natural detergency for improved cleanliness, and protects against rust and corrosion. It also has excellent low-temperature properties for use over a wide temperature range.

Applications:

  • Aero-derivative gas turbines
Syndustrial Turbine Oil meets the requirements of the following industry and OEM specifications:
  • Allison 501-k, 571-k
  • General Electric GEK 97310, LM Series 500 to 6000
  • Rolls-Royce RB211, Avon, Olympus, Spey and Tyne turbines
  • Solar Turbines ES9-224, Revision W, Class III (Synthesized Ester) Turbine Oil
  • U.S. Military MIL-PRF-23699F, Class STD Synthetic Turbine Oil
Features/Benefits:
  • Outstanding oxidation resistance and thermal stability at high temperatures
  • Excellent low-temperature fluidity
  • High load-carrying capacity
  • Protects against rust and corrosion
  • Natural detergency
  • High flash point for reduced fire/explosion hazard
  • Extended service intervals compared with conventional mineral oil-based lubricants

Information provided by Phillips 66 Lubricants.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 0.994 g/cc
Density 8.28 lb/gal
Viscosity Measurement 132Index
Saybolt Viscosity at 100°F 132 SUS
Saybolt Viscosity at 210°F 43 SUS
Kinematic Viscosity at 40°C (104°F) 25.5 cSt
Kinematic Viscosity at 100°C (212°F) 5.1 cSt
ASTM Color 4.0ASTM D1500
 
Chemical PropertiesOriginal ValueComments
Total Acid Number 0.18[mg KOH/g]; SAE ARP 5088
 
Thermal PropertiesOriginal ValueComments
Pour Point -60.0 °C
Flash Point 266 °CCOC
 
Descriptive Properties
Copper Corrosion1aASTM D130
Foam Test10-0Sequence III, ml, ASTM D892
 5-0Sequence I, ml, ASTM D892
 5-0Sequence II, ml, ASTM D892
Particle Contamination<6NAS 1639

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

WCON5274 / 198527

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.