MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

(Viewing data as-entered. Click here to return)
Materion MoldMAX V® Copper Alloy Rod
Categories: Metal; Nonferrous Metal; Copper Alloy

Material Notes: MoldMAX V (MMV) Alloy is a high conductivity, moderately high strength, copper nickel silicon chromium alloy. Applications include injection mold and blow mold cores and cavities.

Information supplied by Materion.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 8.69 g/cc
 
Mechanical PropertiesOriginal ValueComments
Hardness, Brinell >= 250
@Diameter 100 - 125 mm
3000 kgf
 >= 265
@Diameter 12.5 - 89.0 mm
3000 kgf
Hardness, Rockwell C >= 27
@Diameter 12.5 - 89.0 mm
Tensile Strength, Ultimate >= 790 MPa
@Diameter 100 - 125 mm
 >= 860 MPa
@Diameter 12.5 - 89.0 mm
Tensile Strength, Yield >= 725 MPa
@Diameter 100 - 125 mm,
Strain 0.2 %
 >= 790 MPa
@Diameter 12.5 - 89.0 mm,
Strain 0.2 %
Elongation at Break >= 5.0 %
@Diameter 100 - 125 mm
 >= 7.0 %
@Diameter 12.5 - 89.0 mm
Modulus of Elasticity 130 GPa
Fatigue Strength 275 MPa
@Diameter 12.5 - 125 mm,
# of Cycles 1.00e+7
R = -1
Impact Test 7.00 J
@Diameter 12.5 - 125 mm
 
Thermal PropertiesOriginal ValueComments
CTE, linear 17.5 µm/m-°C
Specific Heat Capacity 0.410 J/g-°C
@Temperature 100 °C
Thermal Conductivity 160 W/m-K
@Temperature 100 °C
Melting Point >= 980 °C
Solidus 980 °C
 
Component Elements PropertiesOriginal ValueComments
Chromium, Cr 0.60 - 1.2 %
Copper, Cu 88.7 - 91.5 %As Balance
Nickel, Ni 6.4 - 7.6 %
Silicon, Si 1.5 - 2.5 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Materion PROtherm® Beryllium Copper Alloy
Ampco Metal AMPCOLOY® 95 Cobalt-Copper Alloy, Extrusion, >50.8 mm.
Materion MoldMAX V® Copper Alloy Plate
ArcelorMittal 180 BH Bake hardening steel, Cold rolled
ArcelorMittal IF 180 High strength IF steel, Cold rolled

NBBC19d / 192246

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.