MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Syensqo (Solvay Specialty Polymers) Amodel® AFA-6133 V0 Z PPA, 33% glass fiber
Categories: Polymer; Thermoplastic; Polyphthalamide (PPA); Polyphthalamide (PPA), 30% Glass Fiber Reinforced

Material Notes: 33% glass fiber, flame retardant, high flow, hot-water molds

Amodel® AFA-6133 V0 Z is a 33% glass-fiber reinforced, flame retardant grade of polyphthalamide (PPA) resin specifically formulated for connector applications requiring compatibility with both infrared and vapor phase soldering operations typically used by the electronics industry.

Amodel® AFA-6133 V0 Z offers high flow and short molding cycles, thereby enhancing molding productivity and lowering costs.

- Black: AFA-6133 V0 Z BK 324

Applications: Automotive Applications; Automotive Electronics; Bobbins; Connectors; Electrical/Electronic Applications

Features: Chemical Resistant; Flame Retardant; Good Dimensional Stability; Good Electrical Properties; Good Stiffness; High Flow; High Strength; Hot Water Moldability

Injection notes: Injection Rate: 3 to 4 in/sec
Holding Pressure: 50% of injection pressure
Storage:
- Amodel® compounds are shipped in moisture-resistant packages at moisture levels according to specifications. Sealed, undamaged bags should be preferably stored in a dry room at a maximum temperature of 50°C (122°F) and should be protected from possible damage. If only a portion of a package is used, the remaining material should be transferred into a sealable container. It is recommended that Amodel® resins be dried prior to molding following the recommendations found in this datasheet and/or in the Amodel® processing guide.

Information provided by Solvay Specialty Polymers.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.68 g/ccMethod A; ISO 1183
Water Absorption 0.20 %
@Time 86400 sec
ASTM D570
Linear Mold Shrinkage, Flow 0.0030 cm/cmASTM D955
Linear Mold Shrinkage, Transverse 0.0060 cm/cmASTM D955
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength 199 MPaASTM D638
Tensile Strength, Yield 63.4 MPa
@Temperature 175 °C
ISO 527-2
 75.2 MPa
@Temperature 150 °C
ISO 527-2
 114 MPa
@Temperature 100 °C
ISO 527-2
 186 MPa
@Temperature 23.0 °C
ISO 527-2
Elongation at Break 1.7 %ASTM D638
 1.6 %
@Temperature 23.0 °C
ISO 527-2
 2.4 %
@Temperature 100 °C
ISO 527-2
 4.9 %
@Temperature 175 °C
ISO 527-2
 5.1 %
@Temperature 150 °C
ISO 527-2
Tensile Modulus 16100 MPaASTM D638
 5100 MPa
@Temperature 175 °C
ISO 527-2
 5930 MPa
@Temperature 150 °C
ISO 527-2
 9170 MPa
@Temperature 100 °C
ISO 527-2
 14500 MPa
@Temperature 23.0 °C
ISO 527-2
Flexural Strength 224 MPaASTM D790
 87.6 MPa
@Temperature 175 °C
ISO 178
 101 MPa
@Temperature 150 °C
ISO 178
 161 MPa
@Temperature 100 °C
ISO 178
 259 MPa
@Temperature 23.0 °C
ISO 178
Flexural Modulus 13100 MPaASTM D790
 4620 MPa
@Temperature 175 °C
ISO 178
 4960 MPa
@Temperature 150 °C
ISO 178
 8070 MPa
@Temperature 100 °C
ISO 178
 12600 MPa
@Temperature 23.0 °C
ISO 178
Compressive Strength 145 MPaASTM D695
Shear Strength 80.0 MPaASTM D732
Izod Impact, Notched 85.0 J/mASTM D256
Izod Impact, Unnotched 690 J/mASTM D256
Izod Impact, Notched (ISO) 8.20 kJ/m²Type 1, Notch A; ISO 180
Izod Impact, Unnotched (ISO) 44.0 kJ/m²Type 1; ISO 180
Charpy Impact Unnotched 46.0 kJ/m²Type 1, Edgewise; ISO 179
Charpy Impact, Notched 14.0 kJ/m²Type 1, Edgewise, Notch A; ISO 179
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+15 ohm-cmASTM D257
Surface Resistance 1.00e+15 ohmASTM D257
Dielectric Constant 4.1
@Frequency 1e+6 Hz
ASTM D150
 4.4
@Frequency 100000 Hz
ASTM D150
Dielectric Strength 24.0 kV/mm
@Thickness 3.18 mm
ASTM D149
Dissipation Factor 0.011
@Frequency 1e+6 Hz
ASTM D150
Comparative Tracking Index 400 - 599 VPLC 1; UL 746
Hot Wire Ignition, HWI >= 120 secPLC 0; UL 746
High Amp Arc Ignition, HAI >= 120 arcsPLC 0; UL 746
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 7.00 µm/m-°C
@Temperature 100 - 200 °C
ASTM E831
 17.0 µm/m-°C
@Temperature 0.000 - 100 °C
ASTM E831
CTE, linear, Transverse to Flow 64.0 µm/m-°C
@Temperature 0.000 - 100 °C
ASTM E831
 110 µm/m-°C
@Temperature 100 - 200 °C
ASTM E831
Melting Point 310 °CPeak; ASTM D3418
 310 °CISO 11357-3
Deflection Temperature at 1.8 MPa (264 psi) 277 °CAnnealed; ASTM D648
 282 °CUnannealed, Flatwise; ISO 75-2/A
Flammability, UL94 V-0
@Thickness 0.800 mm
 
Processing PropertiesOriginal ValueComments
Rear Barrel Temperature 327 - 332 °C
Middle Barrel Temperature 316 - 324 °C
Front Barrel Temperature 316 - 324 °C
Melt Temperature 321 - 338 °CInjection
Mold Temperature 66.0 - 93.0 °C
Drying Temperature <= 120 °C
@Time 14400 sec
Moisture Content 0.030 - 0.060 %Injection
 
Descriptive Properties
AdditiveFlame Retardant
AvailabilityAsia Pacific
 Europe
 Latin America
 North America
ColorBlack
FormsPellets
Part Marking Code [ISO 11469]>PA6T/66-GF33<
ProcessingWater-Heated Mold Injection Molding
Resin ID [ISO 1043]PA6T/66 GF33 FR(17)
RoHS ComplianceYes

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSOL8Y4077 / 279877

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.