MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Eastman Eastar DN011 Copolyester
Categories: Polymer; Thermoplastic; Polyester, TP

Material Notes: Eastar Copolyester DN011 is a brilliantly clear polymer having excellent impact strength, chemical resistance, and low shrinkage rates. Eastar Copolyester DN011 contains a mold release.

Applications/Uses

  • Cosmetic jar caps
  • Cosmetic jars
  • Displays
  • Floor care
  • Fragrance caps
  • Lipstick containers
  • Personal Care and Cosmetics
  • Refrigerator interior components
  • Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
     
    Physical PropertiesOriginal ValueComments
    Specific Gravity 1.23 g/ccASTM D792
    Linear Mold Shrinkage 0.0020 - 0.0050 cm/cmASTM D955
     
    Mechanical PropertiesOriginal ValueComments
    Hardness, Rockwell R 105ASTM D785
    Tensile Strength at Break 54.0 MPaASTM D638
    Tensile Strength, Yield 44.0 MPaASTM D638
    Elongation at Break 330 %ASTM D638
    Elongation at Yield 4.0 %ASTM D638
    Tensile Modulus 1.80 GPaASTM D638
    Flexural Strength 66.0 MPaASTM D790
    Flexural Modulus 1.80 GPaASTM D790
    Izod Impact, Notched 0.770 J/cm
    @Temperature -40.0 °C
    ASTM D256
     NB
    @Temperature 23.0 °C
    ASTM D256
    Izod Impact, Unnotched NBASTM D4812
     NB
    @Temperature -40.0 °C
    ASTM D4812
    Puncture Energy 46.0 JPuncture Resistance @Max Load, 23°C; ASTM D3763
     46.0 J
    @Temperature -40.0 °C
    Puncture Resistance at Max Load; ASTM D3763
     
    Thermal PropertiesOriginal ValueComments
    Deflection Temperature at 0.46 MPa (66 psi) 73.0 °CASTM D648
    Deflection Temperature at 1.8 MPa (264 psi) 64.0 °CASTM D648
     
    Optical PropertiesOriginal ValueComments
    Haze 1.4 %ASTM D1003
    Transmission, Visible 89 %Regular Transmittance; ASTM D1003
     92 %Total Transmittance; ASTM D1003
     
    Processing PropertiesOriginal ValueComments
    Melt Temperature 249 - 271 °C
    Mold Temperature 16.0 - 38.0 °C
    Drying Temperature 71.0 °C
    Dry Time 6 hour

    Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

    Users viewing this material also viewed the following:
    Overview of materials for PCTG Copolyester
    Eastman Eastar 5445 PCTG Copolyester, Film
    Eastman Eastar DN010 Copolyester
    Eastman Eastar DN101 PCTG Copolyester
    Eastman DuraStar DS1000 Polymer, Natural

    PE9029 / 35085

    Aluminum Castings

    Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

    The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.