MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Angst+Pfister APSOplast® PC EC PC + electrically conductive surface coating
Categories: Polymer; Thermoplastic; Polycarbonate (PC)

Material Notes: PC EC is a scratch-resistant polycarbonate characterized by electrically conductive surfaces (surface resistance of 103–105 O) and excellent transparency and translucency as well as high impact resistance and dielectric strength. This challenging combination of properties is always in demand for glazing material in special production areas where electrostatic charging must be avoided.

Information provided by Angst + Pfister

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.20 g/cc0.0434 lb/in³DIN EN ISO 1183-1
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 60.0 MPa8700 psi50 mm/min; DIN EN ISO 527
Tensile Strength, Yield 60.0 MPa8700 psi50 mm/min; DIN EN ISO 527
Elongation at Break 70 %70 %50 mm/min; DIN EN ISO 527
Elongation at Yield 6.0 %6.0 %50 mm/min; DIN EN ISO 527
Modulus of Elasticity 2.40 GPa348 ksi1 mm/min; DIN EN ISO 527
Flexural Strength 100 MPa14500 psi2 mm/min; ISO 178
Charpy Impact Unnotched NBNBDIN EN ISO 179-1eU
Charpy Impact, Notched 1.10 J/cm²5.23 ft-lb/in²DIN EN ISO 179-1eA
 
Electrical PropertiesMetricEnglishComments
Surface Resistance 1e+05 - 1.00e+7 ohm1e+05 - 1.00e+7 ohmIEC 60093
Dielectric Constant 1212IEC 60250
 
Thermal PropertiesMetricEnglishComments
CTE, linear 65.0 µm/m-°C36.1 µin/in-°FDIN 53752
 
Optical PropertiesMetricEnglishComments
Refractive Index 1.5861.586ISO 489
Haze >= 1.0 %>= 1.0 %
Transmission, Visible 89 %
@Thickness 3.00 mm
89 %
@Thickness 0.118 in
DIN 5036 / ASTM D-1003 / ISO 13468-1/-2
 
Descriptive Properties
Colorclear transparent
Light reflectance factor8DIN 5033/5036

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PANGP020 / 250518

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.