MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Lubriplate 1500 Lithium Complex Multi-Purpose Grease
Categories: Fluid; Lubricant; Lithium Gellant

Material Notes: These multi-purpose lithium complex lubricants can withstand higher temperatures than traditional lithium greases. They provide high film strength, excellent shear stability, long lubricant life, and exceptional anti-wear properties. Available in four NLGI densities for a variety of applications. No 1552 is NLGI GC-LB certified.

Applications: Leaky Gear Cases. Trailer wheel bearings.

1500 Series Greases are available in Pails, 1/4 Drums & Drums. No. 1551 & No. 1552 are also available in Cartridges.

Information provided by Lubriplate

Key Words: Part Number L0163-
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Saybolt Viscosity at 100°F 1100 SUS
Kinematic Viscosity at 40°C (104°F) 200 cSt
 
Mechanical PropertiesOriginal ValueComments
Penetration P(0), 1/10 mm 400Unknown Amount of Work
Penetration P(60), 1/10 mm 430Unknown Amount of Work
 
Thermal PropertiesOriginal ValueComments
Minimum Service Temperature, Air -10.0 °FApprox. Cold test
 
Descriptive Properties
Antiwear (AW)/ Extreme Pressure (EP)AW/EP
NLGI Grade00
Rust/Oxidative AdditivesYES
Water ResistantYES

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

WLUBR044 / 76090

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.