MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

DuPont Mobility and Materials BETALINK™ 36 2-component Silane Modified Polymer Adhesive
Categories: Polymer; Thermoset

Material Notes: 2-component, permanently elastic STP based adhesive with a very fast strength build-up and very good adhesion properties on a large variety of substrates. Thanks to fast cross-linking it is possible to bond parts in a continuous working process.

Information provided by DuPont.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.30 - 1.40 g/cc0.0470 - 0.0506 lb/in³Component A
 1.35 - 1.45 g/cc0.0488 - 0.0524 lb/in³Component B
Viscosity  6000 cP
@Shear Rate 10.0 1/s,
Temperature 23.0 °C
6000 cP
@Shear Rate 10.0 1/s,
Temperature 73.4 °F
Component B
 10000 cP
@Shear Rate 10.0 1/s,
Temperature 23.0 °C
10000 cP
@Shear Rate 10.0 1/s,
Temperature 73.4 °F
Component A
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 45 - 5545 - 55DIN 53505
Tensile Strength at Break 3.00 MPa435 psiISO 1798
Elongation at Break 150 %150 %ISO 1798
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air <= 90.0 °C<= 194 °F
 <= 90.0 °C<= 194 °FTemperature stability
 
Processing PropertiesMetricEnglishComments
Processing Temperature 5.00 - 40.0 °C41.0 - 104 °F
Working Life >= 4.00 min>= 4.00 min
 
Descriptive Properties
Basis2-component Silane modified Polymers
ColorLight gray
CompatibilityComposites
 Paint
Mixing ratio1:1 volumetric
PolymerAdhesive
Regional AvailabilityEurope
 Near East/Africa

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PDTF9021e / 290847

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.