Paper phenolic grade with better electrical properties than NP612. NP625 requires slightly more heat to shear and punch than NP612.Information provided by Norplex-Micarta |
Paper, Phenolic, Micarta, NEMA XPC, MIL-I-24768/20 - PBM-PC, ASTM D709 Type I Grade XPC |