MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Eastman Llumar R20 SR CDF (Silver) Window Film
Categories: Polymer; Film

Material Notes: Reflective films feature reflectance on both interiors and exteriors for superior reduction in summer cooling costs and heat retention in winter. Providing a high level of glare and heat control, they are scratch-resistant, shield 99% of ultraviolet rays, and provide excellent heat rejection.

Information provided by Eastman

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Optical PropertiesOriginal ValueComments
Transmission, Visible 15 %
UV Transmittance 11 %Solar
Reflection Coefficient, Visible (0-1) 0.57Total Solar Reflectance
 0.62Visible Reflectance (exterior)
 0.63Visible Reflectance (interior)
 
Descriptive Properties
% Glare Reduction83
% Summer Solar Heat Gain Reduction77
% Total Solar Energy Rejected80
% Ultraviolet Ray Protection (wavelengths 300-380nm)>99
% Winter Heat Loss Reduction13
Emissivity0.58
Light to solar gain (LSG)0.75
Shading coefficient0.22
Solar absorption32
Solar Heat Gain Coefficient0.2
U-value0.9Winter

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PEATM5414 / 222608

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.