MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

ExxonMobil LL 1001x72 Blown Film Resin  (discontinued **)
Categories: Polymer; Film; Thermoplastic; Polyethylene (PE); Linear Low Density (LLDPE); Linear Low Density Polyethylene (LLDPE), Film Grade

Material Notes: Product Description: LL 1001 are butane LLDPE blown film resins having good draw down. Films made from LL 1001 resins exhibit good tensile and toughness properties.

Availability: Latin America, North America and South America

Additive:

  • Antiblock: 5000 ppm
  • Slip: 850 ppm
  • Processing Aid: No
  • Thermal Stabilizer: Yes
Applications:
  • Agricultural Film
  • Bag in Box
  • Barrier Food Packaging
  • Blown Film
  • Bread Bags
  • Food packaging
  • Form Fill and Seal Packaging
  • Freezer Film
  • Garment Film
  • General Packaging
  • Heavy Duty Bags
  • Ice Bags
  • Industrial Liners
  • Industrial Packaging
  • Lamination Film
  • Liners
  • Multilayer Packaging Film
  • Packaging Films
  • Produce Bags
  • Refuse Bags
  • Shoppers
  • Stand Up Pouches
  • Trash Bags

Information provided by ExxonMobil Chemical

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.918 g/cc0.0332 lb/in³ExxonMobil Method
Melt Flow 1.0 g/10 min
@Load 2.16 kg,
Temperature 190 °C
1.0 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Antiblock Level 5000 ppm5000 ppm
Slip Level 850 ppm850 ppm
 
Mechanical PropertiesMetricEnglishComments
Film Tensile Strength at Yield, MD 9.65 MPa1400 psiASTM D882
Film Tensile Strength at Yield, TD 9.65 MPa1400 psiASTM D882
Film Elongation at Break, MD 580 %580 %ASTM D882
Film Elongation at Break, TD 850 %850 %ASTM D882
Puncture Energy 3.13 J2.31 ft-lbExxonMobil
Elmendorf Tear Strength, MD 3.15 g/micron80.0 g/milASTM D1922
Elmendorf Tear Strength, TD 15.7 g/micron400 g/milASTM D1922
Dart Drop 4.09 g/micron104 g/milASTM D1709
Film Tensile Strength at Break, MD 53.1 MPa7700 psiASTM D882
Film Tensile Strength at Break, TD 35.3 MPa5120 psiASTM D882
1% Secant Modulus, MD 193 MPa28000 psiASTM D882
1% Secant Modulus, TD 223 MPa32300 psiASTM D882
 
Thermal PropertiesMetricEnglishComments
Melting Point 121 °C249 °FPeak Melting Temperature; ExxonMobil Method
 
Optical PropertiesMetricEnglishComments
Haze 15.3 %15.3 %ASTM D1003
Gloss 45 %45 %45°; ASTM D2457
 
Descriptive Properties
FeaturesThermal Stabilizer

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
ExxonMobil LL 3201.69 Premium High Strength Film Resin
ExxonMobil LL 3201.36 Premium High Strength Film Resin
ExxonMobil LLDPE LL 1001X72 Linear Low Density Polyethylene Resin
ExxonMobil LLDPE LL 6201RQ Wire & Cable Linear Low Density Polyethylene Resin (European Grade)
ExxonMobil LLDPE LL 1001.32 Linear Low Density Polyethylene Resin

PEXB190 / 37495

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.