MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Idemitsu Kosan TARFLON NEO™ RC2041 Polycarbonate-PDMS Copolymer
Categories: Polymer; Thermoplastic; Polycarbonate (PC); Siloxane

Material Notes: General information on TARFLON NEO™ PC-PDMS Copolymer (Polydimethylsiloxane): Excellent low-temperature impact ductility at -30°C and below, Superior balance of flow ability and impact strength, Good chemical resistance (Especially good resistant to alkali, compared with standard PC), Long-term stability in physical properties (Especially in weather ability), Good heat-resistance (Same as that of standard PC).

Information provided by Idemitsu Losan Co.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.18 g/cc0.0426 lb/in³ISO 1183(JIS K7112)
Moisture Absorption 0.200 %
@Time 86400 sec
0.200 %
@Time 24.0 hour
50% RH; ISO 62(JIS K7209)
Linear Mold Shrinkage, Flow 0.0060 - 0.0080 cm/cm
@Thickness 2.00 mm
0.0060 - 0.0080 in/in
@Thickness 0.0787 in
Idemitsu Method
Linear Mold Shrinkage, Transverse 0.0060 - 0.0080 cm/cm
@Thickness 2.00 mm
0.0060 - 0.0080 in/in
@Thickness 0.0787 in
Idemitsu Method
Melt Flow 14.16 g/10 min
@Load 1.20 kg,
Temperature 300 °C
14.16 g/10 min
@Load 2.65 lb,
Temperature 572 °F
ISO 1133 (JIS K7210)
Spiral Flow 24.0 cm
@Thickness 2.00 mm
9.45 in
@Thickness 0.0787 in
Width:10mm. Cylinder: 240°C/Mold: 40°C. Inj.Pressure: 125 MPa.; Idemitsu Method
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 59.0 MPa8560 psiISO 527-1,2 (JIS K7161, 7162)
Elongation at Break 110 %110 %Nominal; ISO 527-1,2 (JIS K7161, 7162)
Flexural Strength 90.0 MPa13100 psiISO 178 (JIS K7171)
Flexural Modulus 2.20 GPa319 ksiISO 178 (JIS K7171)
Izod Impact, Notched  6.00 J/cm
@Temperature -30.0 °C
11.2 ft-lb/in
@Temperature -22.0 °F
ASTM D256
 7.50 J/cm
@Temperature 0.000 °C
14.1 ft-lb/in
@Temperature 32.0 °F
ASTM D256
 8.00 J/cm
@Temperature 23.0 °C
15.0 ft-lb/in
@Temperature 73.4 °F
ASTM D256
Charpy Impact, Notched  2.50 J/cm²
@Temperature -30.0 °C
11.9 ft-lb/in²
@Temperature -22.0 °F
ISO 179-1(JIS K7111)
 8.00 J/cm²
@Temperature 23.0 °C
38.1 ft-lb/in²
@Temperature 73.4 °F
ISO 179-1(JIS K7111)
 
Thermal PropertiesMetricEnglishComments
CTE, linear 70.0 µm/m-°C38.9 µin/in-°FISO 11359-2
Deflection Temperature at 1.8 MPa (264 psi) 123 °C253 °FISO 75-1,2 (JIS K7191-1,2)
 
Optical PropertiesMetricEnglishComments
Transmission, Visible 86 %86 %Total Luminous; ISO 13468-1 (JIS K7361-1)
 
Processing PropertiesMetricEnglishComments
Melt Temperature 270 - 310 °C518 - 590 °FCylinder Temperature
 <= 320 °C<= 608 °FMax Cylinder Temperature
Mold Temperature 80.0 - 110 °C176 - 230 °F
Drying Temperature 120 °C
@Time 18000 - 28800 sec
248 °F
@Time 5.00 - 8.00 hour

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PIDEM208 / 249572

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.