System Message
Advertise with MatWeb!
Data sheets for over
180,000
metals, plastics, ceramics, and composites.
HOME
•
SEARCH
•
TOOLS
•
SUPPLIERS
•
FOLDERS
•
ABOUT US
•
FAQ
•
LOG IN
Recently Viewed Materials (most recent at top)
Login
to see your most recently viewed materials here.
Or if you don't have an account with us yet, then
click here to register.
Searches:
Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
(Viewing data as-entered.
Click here
to return)
Ter Hell Plastic K-Resin KRE 9902 Butadiene-Styrene Copolymer
Categories:
Polymer
;
Thermoplastic
;
Styrene-Butadiene
;
Styrene-Butadiene Copolymer, SBC
Material Notes:
Description:
Butadiene-Styrene Copolymer Compound, good transparency with impact strength and stiffness well-balanced.
Application:
For all kinds of injection molded parts.
Information provided by Ter Hell Plastic GMBH.
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Original Value
Comments
Specific Gravity
1.02
g/cc
ISO 1183
Melt Flow
7.0
g/10 min
@Load 5.00 kg,
Temperature 200 °C
ISO 1133
Mechanical Properties
Original Value
Comments
Tensile Strength, Yield
30.0
MPa
dry; ISO 527
Elongation at Break
30 %
dry; ISO 527
Elongation at Yield
5.0 %
dry; ISO 527
Tensile Modulus
2000
MPa
dry; ISO 527
Charpy Impact Unnotched
13.0
kJ/m²
dry; ISO 179
Charpy Impact, Notched
2.00
kJ/m²
dry; ISO 179
Thermal Properties
Original Value
Comments
Vicat Softening Point
75.0
°C
B/50; ISO 306
95.0
°C
A/50; ISO 306
Flammability, UL94
HB
@Thickness 3.20 mm
Processing Properties
Original Value
Comments
Processing Temperature
190
-
230
°C
Drying Temperature
60.0
°C
Dry Time
2
-
4
hour
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to go back to viewing the property data in MatWeb's normal format.
Users viewing this material also viewed the following:
I. Stern Q Resin Clear Styrene Butadiene Copolymer
Versalis Europrene Latice® 406 Carboxylated Styrene - Butadiene Copolymer
Overview of materials for Styrene-Butadiene Copolymer, SBC
Chevron Phillips K-Resin® KR99HG Styrene-Butadiene Copolymer, Injection Molding Grade
Avient Gravi-Tech™ GRV-TP-080-W-NAT Styrene Butadiene Block Copolymer (SBC)
PTERH904 / 120642
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
info@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.