MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Chemical Concepts Chem-Set™ C-19 Seaming Adhesive
Categories: Polymer; Adhesive; Thermoset

Material Notes: Ideal for fabricating countertops, bathroom vanities, wall panels, and other surfaces, C19 produces tough, virtually invisible bonds on a variety of surfacing materials including cast polymers, acrylics, polyester blends, engineered quartz, and natural stone. Available in multitude colors, C19 Seaming Adhesives coordinate with all major domestic and international brands of surfacing; both acrylic and polyester. They can also be custom tinted. Depending on the color, they cure to either an opaque or translucent finish. Supplied in convenient cartridges, C19 is mixed in a 10:1 ratio with static nozzles that eliminate premixing, pot-life concerns, cleanup, and waste. Adhesives are UV-stable, Greenguard certified and all ingredients are European EINECS-compliant. They are 100% reactive and contain no solvents.

FEATURES: -Bonds in Wet Environments. - UV Stable. - High Strength. - Room Temperature Cure. - 100% Reactive. - Excellent Wear Resistance. - Industry Standard Packaging.

SUSTAINABILITY GUIDE: - GREENGUARD® Children & Schools Certified. - GREENGUARD® Indoor Air Quality Certified. - Contributes to LEED® and other green building rating.

Information provided by Chemical Concepts™.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 0.930 - 1.05 g/cc0.930 - 1.05 g/ccAdhesive
Density 0.9290 - 1.049 g/cc0.03356 - 0.03790 lb/in³Adhesive
Volatile Organic Compounds (VOC) Content 5.3 g/l5.3 g/lEPA Method 24
Vapor Pressure <= 0.000667 bar<= 0.500 torrActivator
 0.0373 bar28.0 torrAdhesive
 
Mechanical PropertiesMetricEnglishComments
Adhesive Bond Strength 27.6 - 34.5 MPa4000 - 5000 psiNatural Stone, substrate failure
 31.0 - 41.4 MPa4500 - 6000 psiQuartz, substrate failure
 
Thermal PropertiesMetricEnglishComments
Melting Point -47.8 °C-54.0 °F
Boiling Point 101 °C213 °F
 >= 288 °C>= 550 °FActivator
Flash Point 10.0 °C50.0 °FTag CC. Fine mists explosive below flash point.
 
Descriptive Properties
AppearanceAdhesive: paste. Activator: liquid
Auto Ignition Temperature790°F
Colorvarious
Evaporation Point<1 (butyl acetate =1). Activator
 3. Adhesive
Flammability Limits1.7 to 12.5%
OdorAdhesive: fragrant. Activator: Mild Ester.
Vapor Density3.5 (air=1)

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PCHEMI931 / 232167

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.