MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Arkema ORGASOL® 2002 ES6 NAT 3 Polyamide 12
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 12 (PA12)

Material Notes: Information provided by Arkema Group

Key Words: 2002 ES 6 Nat 3
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Apparent Bulk Density 0.425 g/ccUnpacked; ISO 1068
Particle Size >= 40 µmFine Particles; < 10% less than 40 µm; ISO 13319
 <= 80 µmISO 13319
Specific Surface Area 1.0 m²/gISO 9277
Thickness 60.0 micronsMedian; ISO 13319
 
Thermal PropertiesOriginal ValueComments
Melting Point 177 °CISO 11357-3
 
Descriptive Properties
AppearanceWhite spheroidal powder
Form as DeliveredPowder
Moisture SensitiveNo

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
LG Chemical SEETEC M1400 Polypropylene Impact Copolymer
Arkema ORGASOL® 2002 ES4 NAT 3 Polyamide 12
Arkema ORGASOL® 2002 ES3 Nat 3 Polyamide 12
Kingfa PA6-G30 N101 30% Glass Fiber Reinforced PA6 (general purpose)
Evonik VESTOSINT® 1141 colored Polyamide 12

PARKG481 / 24519

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.