Total CD 471 HDPE conduit
Categories:
Polymer
;
Thermoplastic
;
Polyethylene (PE)
;
High Density (HDPE)
;
High Density Polyethylene (HDPE), Pipe Grade
Material Notes:
Applications: Wire and cable conduit, fiber optic innerduct
Information provided provided by Total Petrochemicals.
Total Petrochemicals acquired former Fina and Atofina plastics product lines.
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Metric
English
Comments
Density
0.947
g/cc
0.0342
lb/in³
ASTM D 792
Environmental Stress Crack Resistance
>=
500
hour
>=
500
hour
ASTM D1693 cond. B 10% lgepal
>=
1000
hour
>=
1000
hour
ASTM D1693 cond. C 100% lgepal
Melt Flow
0.28
g/10 min
@Load 2.16 kg
0.28
g/10 min
@Load 4.76 lb
ASTM D 1238
High Load Melt Index
20
g/10 min
@Load 21.6 kg
20
g/10 min
@Load 47.6 lb
ASTM D 1238
Mechanical Properties
Metric
English
Comments
Hardness, Shore D
63
63
ASTM D 2240
Tensile Strength, Yield
>=
22.8
MPa
>=
3300
psi
ASTM D 638 type IV
Elongation at Break
>= 600 %
>= 600 %
ASTM D 638 type IV
Flexural Modulus
0.793
GPa
115
ksi
ASTM D 790
Thermal Properties
Metric
English
Comments
CTE, linear
180
µm/m-°C
@Temperature 20.0 °C
100
µin/in-°F
@Temperature 68.0 °F
ASTM D 696
Melting Point
126
°C
259
°F
ASTM D3417
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to view all the property values for this datasheet as they were originally entered into MatWeb.
Users viewing this material also viewed the following:
NOVA Chemicals Novapol® HB-W747-A HDPE Extrusion Resin
Total 3802 B HDPE, cable, sheet, pipe, injection molding
Total HP 401N Natural HDPE, pipe
ExxonMobil BU46-060 High Density Polyethylene Resin
ExxonMobil BU46-055 High Density Polyethylene Resin
PFINAP116 / 38699
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
info@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.