MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Imerys NYGLOS® 2 Wollastonite  (discontinued **)
Categories: Ceramic; Oxide; Silicon Oxide; Other Engineering Material; Additive/Filler for Polymer

Material Notes: Wollastonite (calcium metasilicate, or CaSiO3) is a naturally occurring white, non-metallic mineral with an acicular or needle-shaped crystal structure. This distinctive property makes wollastonite an ideal performance mineral for a broad range of industrial and consumer applications.

Composition Notes: Willsboro typical values are reported. Theoretical 48.30 wt% CaO and 51.70 wt% SiO2

.Information provided by NYCO Minerals, subsequently acquired by Imerys.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 2.90 g/cc
Bulk Density 12.5 lb/ft³loose
 25.0 lb/ft³Tapped
Brightness 92 %G.E. Brightness
Oil Absorption 60 %
Solubility of Water 0.0095 %
Particle Size 2.5 µmD50
pH 9.910% Slurry
Molecular Weight 116 g/mol
 
Mechanical PropertiesOriginal ValueComments
Hardness, Mohs 4.5
 
Thermal PropertiesOriginal ValueComments
CTE, linear 6.50 µm/m-°C
@Temperature 20.0 °C
Melting Point 1410 °CASTM D1857
 1540 °Ctheoretical
 
Optical PropertiesOriginal ValueComments
Refractive Index 1.63
 
Component Elements PropertiesOriginal ValueComments
Al2O3 0.34 %
CaO 46.15 %
Fe2O3 0.77 %
K2O 0.050 %
Loss on Ignition(%) 0.50 %
MgO 0.38 %
MnO 0.16 %
SiO2 51.6 %
TiO2 0.050 %
 
Descriptive Properties
AppearanceWhite
Aspect Ratio (L/D)5:1
MorphologyAcicular

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Malvern Minerals Wollastokup® FF Silane Treated Wollastonite
Malvern Minerals Novacite® Daper Untreated Lamellar Quartz Filler/Extender
Imerys ULTRAFIBRE® II Wollastonite
Imerys NYAD® G Special Wollastonite
Imerys 10 AS WOLLASTOCOAT® Wollastonite

CNYCO00 / 1682

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.