MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Akrochem Accelerator DPG
Categories: Other Engineering Material

Material Notes: Product Description: Accelerator DPG is useful as an accelerator/activator for natural rubber, SBR and NBR. It activates accelerators such as MBT, MBTS and sulfenamides. It is a strong secondary for CBTS, BBTS, OBTS, MBT and MBTS. DPG requires the use of zinc oxide and fatty acids. DPG provides satisfactory processing safety and storage stability to rubber compounds. In light colored goods, it causes a brown discoloration and is not recommended for use in compounds that have contact with food (imparts bitter taste). For best aging results, an antioxidant is required. Suggested dosages of DPG in combination with zinc oxide, stearic acid, and sulfur are as follows:
Natural Rubber: 0.10- 0.50 phr with sulfenamides or MBTS
SBR: 0.20 - 0.75 phr with sulfenamides, MBTS or MBT
NBR: 0.20 - 0.50 phr with CBTS, MBTS

Information provided by Akrochem Corporation

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.18 g/cc1.18 g/ccpowder
 1.20 g/cc1.20 g/ccpellets
Ash <= 0.40 %<= 0.40 %
 
Thermal PropertiesMetricEnglishComments
Melting Point >= 143 °C>= 289 °F
 
Descriptive Properties
Appearanceoff-white powder

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PAKZCH437 / 315355

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.