MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Lubrizol PEARLSTICK™ 5702 F3 Thermoplastic Polyurethane
Categories: Polymer; Thermoplastic; Polyurethane, TP

Material Notes: Type: Pearlstick™ 5702 F3 is an aromatic polyester-based thermoplastic polyurethane.

Main Application: Solution coating.

Information provided by The 159 Corporation

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.19 g/cc1.19 g/ccISO 2781
Brookfield Viscosity 180 - 460 cP180 - 460 cP15% Total Solids in THF, Spindle nº 2, 20 rpm
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 6565ISO 868
Tensile Strength 37.0 MPa5370 psiISO 527-2/5A/200
Elongation at Break 590 %590 %ISO 527-2/5A/200
50% Modulus 2.00 MPa
@Strain 50 %
2.00 MPa
@Strain 50 %
ISO 527-2/5A/200
100% Modulus 2.00 MPa
@Strain 100 %
290 psi
@Strain 100 %
ISO 527-2/5A/200
300% Modulus 5.00 MPa
@Strain 300 %
725 psi
@Strain 300 %
ISO 527-2/5A/200
Tear Strength 45.0 kN/m257 pliUnnicked; ISO 34-1B
 
Thermal PropertiesMetricEnglishComments
Melting Point 73.0 °C163 °FKofler

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PLUBR5053 / 238923

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.