MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Momentive Performance Materials Type 219 Fused Quartz Tubing  (discontinued **)
Categories: Ceramic; Glass; Oxide; Silicon Oxide

Material Notes: Known as "Ozone-Free" or "Germicidal" quartz tubing. Transmits UV-A and UV-B while blocking the deep, high energy wavelengths that cause ozone generation and pose the greatest exposure risks. Transmits the 253.7 nm mercury emission very efficiently, making it an ideal material for disinfecting applications and various other UV treatments. Softening point 1660°C. Annealing point 1204°C. Strain point 1106°C.

Data provided by GE Quartz.

GE Quartz became a part of Momentive Performance Materials in 2006.

Key Words: Quartz Tubes
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 2.21 g/cc
Viscosity 5.60e+14 cP
@Temperature 1100 °C
 
Mechanical PropertiesOriginal ValueComments
Knoop Microhardness 570kg/mm²
Hardness, Mohs 5.5 - 6.5(Type 214)
Modulus of Elasticity 75.0 GPaYoung's Modulus
Compressive Strength 94.0 MPadesign compressive strength
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 2.50e+10 ohm-cm
@Temperature 350 °C
Dielectric Constant 5.8
@Frequency 1e+6 Hz
 
Thermal PropertiesOriginal ValueComments
CTE, linear 0.400 µm/m-°C
@Temperature 20.0 °C
 0.450 µm/m-°C
@Temperature 1000 °C
 0.600 µm/m-°C
@Temperature 500 °C
 0.700 µm/m-°C
@Temperature 250 °C
Specific Heat Capacity 0.700 J/g-°C
@Temperature 0.000 - 50.0 °C
Thermal Conductivity 1.40 W/m-K
Softening Point 1660 °C
Annealing Point 1204 °C
Strain Point 1106 °C
 
Optical PropertiesOriginal ValueComments
Refractive Index 1.456
Transmission, Visible 92 %Entire visible spectrum; 1 mm thickness (includes surface reflection losses)
IR Transmittance 93 %
@Wavelength <=2500 nm,
Thickness 1.00 mm
Very wavelength dependent - drop begins above 2500 nm and cutoff almost complete at 4200 nm; (includes surface reflection losses)
UV Transmittance 0.00 %
@Wavelength <=220 nm,
Thickness 1.00 mm
Highly wavelength dependent - cutoff below 220 nm; (includes surface reflection losses)
 
Descriptive Properties
ColorClear

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Momentive Performance Materials Type 214 Fused Quartz Tubing
Ceradyne Thermo-Sil® UHS Fused Silica
Momentive Performance Materials Type 254 Fused Quartz Tubing
Quartz (SiO2)
Fused Quartz

CGEQ19 / 895

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.