MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

UBE Tyranno Grade ZMI Ceramic High Temperature Fiber
Categories: Ceramic; Oxide; Other Engineering Material; Composite Fibers

Material Notes: Tyranno ZMI Fiber is the continuous ceramic fiber consisting of Si, Zr,C and O. Advanced composites reinforced by the Tyranno Fiber are used in the environmental preservation field in the future such as ultra high speed transportation, energy savings, CO2 and NOx reduction, and purification of the exhaust fumes. The reinforcing fibers need to meet the demand for these applications such as high temperature stability, high strength, and high reliability in the extreme environment. ZMI-grade fiber which contains Zirconium has improved its stability and oxidation resistance at high temperatures comparing with ordinary type of Tyranno Fibers which contain Titanium.

Information provided by UBE.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 2.48 g/cc0.0896 lb/in³
Filament Diameter 11 µm11 µm
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate 3400 MPa493000 psi
Elongation at Break 1.7 %1.7 %
Tensile Modulus 195 GPa28300 ksi
 
Thermal PropertiesMetricEnglishComments
CTE, linear 4.00 µm/m-°C
@Temperature 20.0 - 1000 °C
2.22 µin/in-°F
@Temperature 68.0 - 1830 °F
Specific Heat Capacity 0.709 J/g-°C0.169 BTU/lb-°F
Thermal Conductivity 2.50 W/m-K17.4 BTU-in/hr-ft²-°F
Maximum Service Temperature, Inert 1900 °C3450 °F
 
Component Elements PropertiesMetricEnglishComments
Carbon, C 34 %34 %
Oxygen, O 9 %9 %
Silicon, Si 56 %56 %
Zirconium, Zr 1 %1 %
 
Descriptive Properties
Number of Filaments800 fil./yarn
Structureamorphous
Tex200 g/1000m

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Materion Vit 106a Zirconium-Based Bulk Metallic Glass (BMG)
UBE Tyranno Grade SA Ceramic High Temperature Fiber
Materion Vit 105 Zirconium-Based Bulk Metallic Glass (BMG)
Materion Vit 601 Zirconium-Based Bulk Metallic Glass (BMG)
Grade 706 Zirconium (Zr-2.5Nb)

CUBE250 / 2731

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.