MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Zoltek™ PX30 KF07 Carbon Fiber Knit Fabric
Categories: Carbon; Carbon Fiber/Carbon Fibre; Other Engineering Material; Composite Fibers

Material Notes: ZOLTEK PX30 Low-Oxidation Knitted Carbon Fabric is high modulus fiber fabric made from spun yarn. The fabric has a jersey knit construction, which will conform to multiple curvatures. Thermal oxidative and dimensional stabilities are attained during heat treatment. Applications include thermal protection systems, such as, heat shields, rocket nozzles, and carbon/carbon brakes.

Information provided by Zoltek Corporation.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.75 g/cc0.0632 lb/in³
Thickness 1000 microns39.4 milCured
 
Component Elements PropertiesMetricEnglishComments
Carbon, C 99 %99 %
 
Descriptive Properties
Areal Weight250g/m2
ConstructionSingle knit jersey
Oxidation Rate1% per hour @ 932°F
Roll Length14.63 m, (minimum)
Roll Width51 cm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Solvay Thornel® T-650/35 6K Carbon Fiber, Polyacrylonitrile (PAN) Precursor
VICTREX™ PEEK 450CA40 Polyetheretherketone, 40% Carbon Fibre Reinforced
Graphite, Carbon, C
Zoltek™ PX35 UD500 Uni-Directional Carbon Fabric
Aremco Graphi-Bond™ 551-R

ECZO830 / 232302

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.