MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
ASTM A231 Alloy Steel Wire
Categories: Metal; Ferrous Metal; Alloy Steel; Low Alloy Steel; ASTM Steel; Carbon Steel; Medium Carbon Steel

Material Notes: Round, chromium-vanadium, alloy steel wire for manufacturing springs used at elevated temperature

Key Words: UNS K15048
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 7.80 g/ccTypical of ASTM Steel
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Ultimate 1310 - 1450 MPa
@Diameter 12.7 mm
 1340 - 1480 MPa
@Diameter 11.1 mm
 1380 - 1520 MPa
@Diameter 9.53 mm
 1400 - 1540 MPa
@Diameter 7.92 mm
 1410 - 1550 MPa
@Diameter 7.19 mm
 1450 - 1590 MPa
@Diameter 6.20 mm
 1520 - 1650 MPa
@Diameter 4.88 mm
 1550 - 1690 MPa
@Diameter 4.11 mm
 1620 - 1760 MPa
@Diameter 3.43 mm
 1690 - 1830 MPa
@Diameter 2.67 mm
 1760 - 1900 MPa
@Diameter 2.00 mm
 1830 - 2000 MPa
@Diameter 1.60 mm
 1860 - 2030 MPa
@Diameter 1.40 mm
 1930 - 2100 MPa
@Diameter 1.00 mm
 2000 - 2170 MPa
@Diameter 0.810 mm
 2070 - 2240 MPa
@Diameter 0.510 mm
Reduction of Area 40 %
@Diameter 4.11 mm
 40 %
@Diameter 4.88 mm
 40 %
@Diameter 6.20 mm
 40 %
@Diameter 7.19 mm
 40 %
@Diameter 7.92 mm
 40 %
@Diameter 9.53 mm
 40 %
@Diameter 11.1 mm
 40 %
@Diameter 12.7 mm
 45 %
@Diameter 2.67 mm
 45 %
@Diameter 3.43 mm
Modulus of Elasticity 200 GPaTypical Carbon Steel
Bulk Modulus 160 GPaTypical for Steel
Poissons Ratio 0.29Typical Carbon Steel
Shear Modulus 80.0 GPaTypical for Steel
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.0000170 ohm-cmTypical Carbon Steel
 
Thermal PropertiesOriginal ValueComments
CTE, linear 12.0 µm/m-°CTypical Carbon Steel
Specific Heat Capacity 0.470 J/g-°CTypical Carbon Steel
Thermal Conductivity 52.0 W/m-KTypical Carbon Steel
 
Component Elements PropertiesOriginal ValueComments
Carbon, C 0.48 - 0.53 %
Chromium, Cr 0.20 - 0.35 %
Iron, Fe 98.03 %as balance
Manganese, Mn 0.70 - 0.90 %
Phosphorus, P <= 0.040 %
Silicon, Si 0.20 - 0.35 %
Sulfur, S <= 0.040 %
Vanadium, V >= 0.15 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
ASTM A232 Alloy Steel Wire
ASTM A229 Oil-tempered Steel Wire, Class II
ASTM A227 Steel Wire, Class I
ASTM A401 Alloy Steel Wire
ASTM A229 Oil-tempered Steel Wire, Class I

MSA231 / 142772

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.