  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

BRP Manufacturing BC715 Neoprene Rubber Sheet
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE)

Material Notes: Material: Neoprene Rubber Sheet
BRP Style: BC715
Finish: Smooth (Fabric Finish is Available)
ASTM Callout: ASTM D2000 2BC715A14B14C12EO34F17

Information provided by BRP Manufacturing Company

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength >= 10.3 MPa>= 1500 psiOriginal; ASTM D412
 <= 3.10 MPa
@Temperature 100 °C,
Time 252000 sec
<= 450 psi
@Temperature 212 °F,
Time 70.0 hour
EO34, Fluid Resistance, 903 Oil; ASTM D471IRM
 <= 8.791 MPa
@Temperature 100 °C,
Time 252000 sec
<= 1275 psi
@Temperature 212 °F,
Time 70.0 hour
A14 – Heat Resistance; ASTM D573
 7.24 - 13.4 MPa
@Temperature 100 °C,
Time 252000 sec
1050 - 1950 psi
@Temperature 212 °F,
Time 70.0 hour
Heat Aged; ASTM D573
Elongation at Break 350 %350 %Original; ASTM D412
 <= 157.5 %
@Temperature 100 °C,
Time 252000 sec
<= 157.5 %
@Temperature 212 °F,
Time 70.0 hour
EO34, Fluid Resistance, 903 Oil; ASTM D471IRM
 <= 175 %
@Temperature 100 °C,
Time 252000 sec
<= 175 %
@Temperature 212 °F,
Time 70.0 hour
Heat Aged; ASTM D573
 <= 210 %
@Temperature 100 °C,
Time 252000 sec
<= 210 %
@Temperature 212 °F,
Time 70.0 hour
A14 – Heat Resistance; ASTM D573
Compression Set  <= 35 %
@Temperature 100 °C,
Time 79200 sec
<= 35 %
@Temperature 212 °F,
Time 22.0 hour
ASTM D395 Method B
 <= 80 %
@Temperature 100 °C,
Time 79200 sec
<= 80 %
@Temperature 212 °F,
Time 22.0 hour
ASTM D395 S
 
Descriptive Properties
Hardness55-85Heat Aged, ASTM D573, 70 h @ 100°C
 65-75ASTM D2240
Oil Immersion<120% Volume ChangeASTM D471, IRM 903 Oil, 70 h @ 100°C
Resistance to Ozone100C12, ASTM D1171

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PBRPM009 / 315670

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.