MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Zinc Orthosilicate, Zn2SiO4
Categories: Ceramic; Oxide; Silicon Oxide

Material Notes: CAS Number: 13597-65-4

Physical Form: White Hexagonal Crystals

Key Words: Zn2SiO4
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 4.10 g/cc0.148 lb/in³
Molecular Weight 222.86 g/mol222.86 g/mol
 
Mechanical PropertiesMetricEnglishComments
Hardness, Mohs 5.55.5
 
Thermal PropertiesMetricEnglishComments
Specific Heat Capacity 0.5533 J/g-°C0.1322 BTU/lb-°FCrystal
Melting Point 1509 °C2748 °F
Heat of Formation -1636.7 kJ/mol-1636.7 kJ/molCrystal
 
Optical PropertiesMetricEnglishComments
Refractive Index 1.6911.691na
 1.7191.719nß
 
Descriptive Properties
SolubilityInsoluble in H2O and Diluted Acid
SynonymWillemite

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Zirconium Orthosilicate, ZrSiO4 (Zircon)
Vermiculite, Magnesium Aluminum Iron Silicate
Thorium Orthosilicate, ThSiO4
Strontium Orthosilicate, Sr2SiO4
Steatite (Magnesium Silicon Oxide)

EINOR3389 / 5471

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.