System Message
Advertise with MatWeb!
Data sheets for over
180,000
metals, plastics, ceramics, and composites.
HOME
•
SEARCH
•
TOOLS
•
SUPPLIERS
•
FOLDERS
•
ABOUT US
•
FAQ
•
LOG IN
Recently Viewed Materials (most recent at top)
Login
to see your most recently viewed materials here.
Or if you don't have an account with us yet, then
click here to register.
Searches:
Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
IRPC Polimaxx Polene HI830 Polystyrene
Categories:
Polymer
;
Thermoplastic
;
Polystyrene (PS)
;
Polystyrene, Molded, Unreinforced
Material Notes:
APPLICATIONS:
EXTRUSION APPLICATION, VACUUM SHEET : FOOD PACKAGING ELECTRICAL APPLIANCES, HOUSEHOLD PRODUCT, TOYS, SANITARY, etc.
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Metric
English
Comments
Melt Flow
3.0
g/10 min
@Load 5.00 kg,
Temperature 200 °C
3.0
g/10 min
@Load 11.0 lb,
Temperature 392 °F
ASTM D1238
Mechanical Properties
Metric
English
Comments
Hardness, Rockwell L
82
@Thickness 6.35 mm,
Temperature 23.0 °C
82
@Thickness 0.250 in,
Temperature 73.4 °F
ASTM D785
Tensile Strength, Yield
21.4
MPa
@Temperature 23.0 °C
3100
psi
@Temperature 73.4 °F
ASTM D638
Flexural Yield Strength
41.4
MPa
@Temperature 23.0 °C
6000
psi
@Temperature 73.4 °F
ASTM D790
Flexural Modulus
2.14
GPa
@Temperature 23.0 °C
310
ksi
@Temperature 73.4 °F
ASTM D790
Izod Impact, Notched
0.120
J/cm
@Thickness 6.35 mm,
Temperature 23.0 °C
0.225
ft-lb/in
@Thickness 0.250 in,
Temperature 73.4 °F
ASTM D256
Thermal Properties
Metric
English
Comments
Deflection Temperature at 1.8 MPa (264 psi)
90.0
°C
@Thickness 6.35 mm
194
°F
@Thickness 0.250 in
ASTM D648
Vicat Softening Point
96.0
°C
@Load 1.00 kg,
Thickness 3.17 mm
205
°F
@Load 2.20 lb,
Thickness 0.125 in
ASTM D1525
Flammability, UL94
HB
@Thickness 3.00 mm
HB
@Thickness 0.118 in
Processing Properties
Metric
English
Comments
Processing Temperature
190
-
230
°C
374
-
446
°F
extrusion
Drying Temperature
80.0
-
85.0
°C
@Time 7200 - 10800 sec
176
-
185
°F
@Time 2.00 - 3.00 hour
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to view all the property values for this datasheet as they were originally entered into MatWeb.
Users viewing this material also viewed the following:
American Polymers API 645-21 Polystyrene
Ineos Nova 212 Crystal Polystyrene Low Flow Grade
Ineos Nova 2110 General Purpose Crystal Polystyrene
I. Stern HP-9450 High Impact Polystyrene Extrusion Grade
I. Stern 913 High Impact Polystyrene Extrusion Grade
PIRPC099 / 84076
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
info@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.