Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

NOVA Chemicals NOVAPOL® HB-W555-AC HDPE Blow Molding Resin
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE); High Density Polyethylene (HDPE), Blow Molding Grade

Material Notes:

Hexene Copolymer

Features:

  • Low particle counts
  • Low leaching
  • Excellent long term container storage performance
  • High rigidity
  • Excellent impact strength
  • Excellent ESCR

Additives:

  • Process stabilizer

Applications:

  • High purity chemical packaging
  • High performance packaging for food and flavorings

United States: NOVAPOL HB-W555-AC resin complies with the specifications contained in the U.S. Food and Drug Administration (FDA) regulation 21 CFR 177.1520 for olefin polymers, para. (c) 3.2a, and may thus be used in the United States as an article or component of an article intended for use in contact with food, without temperature or food-type restrictions, subject to technical suitability.

NOVA Chemicals polyethylene resins are biologically and chemically inert.

Information provided by NOVA Chemicals®

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.955 g/cc0.0345 lb/in³ASTM D 792
ESCR 100% Igepal® >= 500 hour>= 500 hourF50, Condition A; ASTM D 1693
Melt Index of Compound 5.0 g/10 min
@Load 21.6 kg,
Temperature 190 °C
5.0 g/10 min
@Load 47.6 lb,
Temperature 374 °F
ASTM D 1238
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 28.0 MPa4060 psiASTM D 638
Elongation at Break 830 %830 %ASTM D 638
Flexural Modulus 1.40 GPa203 ksiASTM D790
Izod Impact, Unnotched 7.20 J/cm
@Thickness 3.20 mm
13.5 ft-lb/in
@Thickness 0.126 in
Tensile Impact Strength 420 kJ/m²200 ft-lb/in²ASTM D 1822
 
Thermal PropertiesMetricEnglishComments
Brittleness Temperature <= -70.0 °C<= -94.0 °FF50, Notched Specimen; ASTM D 746
 
Compliance PropertiesMetricEnglishComments
FDA YesYesSee notes for details.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PNOVB012 / 194620

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.