MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Magnesium ZH62A-T5, Cast
Categories: Metal; Nonferrous Metal; Magnesium Alloy

Material Notes:

Key Words: UNS M16620; Mg
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.86 g/cc0.0672 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Brinell 7070500 kg load, 10 mm ball
Hardness, Knoop 9393Estimated from Brinell
Hardness, Vickers 8080Estimated from Brinell
Tensile Strength, Ultimate 240 MPa34800 psi
 320 MPa
@Temperature -196 °C
46400 psi
@Temperature -321 °F
 330 MPa
@Temperature -78.0 °C
47900 psi
@Temperature -108 °F
 69.0 MPa
@Temperature 315 °C,
Time 601 sec
10000 psi
@Temperature 599 °F,
Time 0.167 hour
tested at elevated temperature
 195 MPa
@Temperature 150 °C,
Time 601 sec
28300 psi
@Temperature 302 °F,
Time 0.167 hour
tested at elevated temperature
Tensile Strength, Yield  200 MPa
@Temperature -78.0 °C
29000 psi
@Temperature -108 °F
 235 MPa
@Temperature -196 °C
34100 psi
@Temperature -321 °F
 170 MPa
@Strain 0.2 %
24700 psi
@Strain 0.2 %
Elongation at Break 4.0 %4.0 %in 50 mm
 1.0 %
@Temperature -196 °C
1.0 %
@Temperature -321 °F
 2.7 %
@Temperature -78.0 °C
2.7 %
@Temperature -108 °F
Creep Strength 17.0 MPa
@Temperature 205 °C,
Time 3.60e+6 sec
2470 psi
@Temperature 401 °F,
Time 1000 hour
0.2% total extension
Modulus of Elasticity  38.0 GPa
@Temperature 315 °C
5510 ksi
@Temperature 599 °F
 40.0 GPa
@Temperature 205 °C
5800 ksi
@Temperature 401 °F
Tensile Modulus 45.0 GPa6530 ksi
Compressive Yield Strength 170 MPa24700 psiat 0.2% offset
Ultimate Bearing Strength 495 MPa71800 psi
Bearing Yield Strength 340 MPa49300 psi
Poissons Ratio 0.300.30
Machinability 100 %100 %Relative Rating, 100=Best
Shear Modulus 17.0 GPa2470 ksi
Shear Strength 165 MPa23900 psi
Charpy Impact 1.02 J0.752 ft-lbV-notch
 1.02 J
@Temperature -78.0 °C
0.752 ft-lb
@Temperature -108 °F
Notched
 1.02 J
@Temperature -196 °C
0.752 ft-lb
@Temperature -321 °F
Notched
Charpy Impact, Unnotched  8.56 J
@Temperature -196 °C
6.31 ft-lb
@Temperature -321 °F
 15.02 J
@Temperature 24.0 °C
11.08 ft-lb
@Temperature 75.2 °F
 18.99 J
@Temperature -78.0 °C
14.01 ft-lb
@Temperature -108 °F
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.00000650 ohm-cm0.00000650 ohm-cm
 
Thermal PropertiesMetricEnglishComments
Heat of Fusion 373 J/g160 BTU/lb
CTE, linear  27.0 µm/m-°C
@Temperature 20.0 - 200 °C
15.0 µin/in-°F
@Temperature 68.0 - 392 °F
Estimated from similar Mg alloys
 27.1 µm/m-°C
@Temperature 0.000 - 100 °C
15.1 µin/in-°F
@Temperature 32.0 - 212 °F
Specific Heat Capacity 0.960 J/g-°C0.229 BTU/lb-°F
Thermal Conductivity 110 W/m-K763 BTU-in/hr-ft²-°F
Melting Point 520 - 630 °C968 - 1170 °F
Solidus 520 °C968 °F
Liquidus 630 °C1170 °F
 
Processing PropertiesMetricEnglishComments
Casting Temperature 750 - 820 °C1380 - 1510 °FSand Casting
 
Component Elements PropertiesMetricEnglishComments
Copper, Cu <= 0.10 %<= 0.10 %
Magnesium, Mg 92 %92 %As Remainder
Nickel, Ni <= 0.010 %<= 0.010 %
Thorium, Th 1.4 - 2.2 %1.4 - 2.2 %
Zinc, Zn 5.2 - 6.2 %5.2 - 6.2 %
Zirconium, Zr 0.50 - 1.0 %0.50 - 1.0 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Magnesium ZC63-T6
Magnesium ZE41A-T5, Cast
Magnesium ZK31-T5, Forgings
Magnesium ZK40A-T5, Extruded
Magnesium ZK51A-T5, Cast

MMZH62 / 12474

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.