VESTAKEEP® i2 P is a medium-viscosity polyether ether ketone (PEEK) powder that is designed for long term human implant applications. Dry properties listed below Industrial Sector: Medical Devices Delivery form: Powder Conformity: Biocompatibility, Medical application Additives: Unfilled Regulatory: US Pharmacopeia Class VI conformity Color: Natural color Chemical Resistance: General chemical resistanceInformation provided by Evonik. |