MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
IRPC Polimaxx Polene 1126NK Polypropylene Homopolymer
Categories: Polymer; Thermoplastic; Polypropylene (PP)

Material Notes: CHARACTERISTICS: GOOD EXTRUDABILITY, LOW GEL CONTAIN HIGH SLIP AND ANTIBLOCK ADDITIVES

APPLICATIONS: TUBULAR BLOW FILM WATER QUENCH FOR GENERAL PURPOSE FILM, FOOD AND PACKAGING BAGS, GARMENT BAGS

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Melt Flow 11 g/10 min
@Load 2.16 kg,
Temperature 230 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 105ASTM D785
Tensile Strength, Yield 35.0 MPaASTM D638
Elongation at Yield 29 %ASTM D638
Flexural Modulus, 1% Secant 1450 MPaASTM D790
Charpy Impact, Notched 0.300 J/cm²
@Temperature 23.0 °C
DIN 53453
 
Thermal PropertiesOriginal ValueComments
Heat Distortion Temperature 100 °CASTM D648
 
Processing PropertiesOriginal ValueComments
Processing Temperature 180 - 220 °C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
IRPC Polimaxx Polene 1100NK Polypropylene Homopolymer
IRPC Polimaxx Polene 1125NA Polypropylene Homopolymer
IRPC Polimaxx Polene 1124NA Polypropylene Homopolymer
Zhejiang Juner JEPPB003 High Glossy PP
Zhejiang Juner PP430R Weatherability PP Series

PIRPC086 / 84063

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.