MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Syensqo (Solvay Specialty Polymers) Lavanta® 5120 BK 368 High Performance (HPP), 20% glass fiber
Categories: Polymer; Thermoplastic; Polyester, TP

Material Notes: 20% glass fiber, high reflectivity, SMT compatible, HB LED packaging

Lavanta® HPP 5120 is a 20% glass fiber reinforced, high-performance polyester (HPP) injection molding grade developed specifically for HB LED packaging applications that utilize surface mount technology. Key performance properties include easy processing, high stiffness and low moisture absorption, giving it excellent reliability for LEDs used in outdoor displays.

-Black: 5120 BK368

Applications: Electrical/Electronic Applications; LEDs

Features: Chemical Resistant; Fast Molding Cycle; High Stiffness; Light Stabilized; Low Moisture Absorption

Information provided by Solvay Specialty Polymers.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.39 g/ccASTM D792
Water Absorption 0.057 %
@Time 86400 sec
ASTM D570
Linear Mold Shrinkage, Flow 0.0050 cm/cmASTM D955
Linear Mold Shrinkage, Transverse 0.014 cm/cmASTM D955
 
Mechanical PropertiesOriginal ValueComments
Tensile Stress 101 MPaISO 527-2
Elongation at Break 1.8 %ISO 527-2
Tensile Modulus 7280 MPaISO 527-2
Flexural Strength 164 MPaISO 178
Flexural Modulus 6360 MPaISO 178
Izod Impact, Notched (ISO) 4.20 kJ/m²Type 1, Notch A; ISO 180
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 17.0 µm/m-°C
@Temperature 150 - 200 °C
ASTM E831
 23.0 µm/m-°C
@Temperature 50.0 - 100 °C
ASTM E831
CTE, linear, Transverse to Flow 72.0 µm/m-°C
@Temperature 0.000 - 50.0 °C
ASTM E831
 110 µm/m-°C
@Temperature 50.0 - 100 °C
ASTM E831
 160 µm/m-°C
@Temperature 100 - 150 °C
ASTM E831
 160 µm/m-°C
@Temperature 150 - 200 °C
ASTM E831
 170 µm/m-°C
@Temperature 200 - 250 °C
ASTM E831
Deflection Temperature at 0.46 MPa (66 psi) 274 °CUnannealed; ISO 75-2/B
Deflection Temperature at 1.8 MPa (264 psi) 241 °CUnannealed; ISO 75-2/A
 
Processing PropertiesOriginal ValueComments
Rear Barrel Temperature 280 - 290 °C
Front Barrel Temperature 300 - 310 °C
Melt Temperature 300 - 320 °CInjection
Mold Temperature 120 - 150 °C
Drying Temperature 120 °C
@Time 14400 sec
Moisture Content <= 0.030 %Injection
 
Descriptive Properties
AvailabilityAsia Pacific
 Europe
 Latin America
 North America
ColorBlack
FormsPellets
ProcessingInjection Molding

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSOL8Y4357 / 280157

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.