MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

3M Dyneon™ FT 2350 Fluoroelastomer
Categories: Polymer; Thermoset; Fluoropolymer, TS; Rubber or Thermoset Elastomer (TSE)

Material Notes: 3M™ Dyneon™ Fluoroelastomer FT 2350 can be compounded using standard water cooled internal mixers or two-roll mills with standard fillers and ingredients utilized in typical fluoroelastomer formulations. The “dry” ingredients should be blended before adding to the masticated gum. For best results, Dyneon FT 2350 should be banded on the mill several minutes prior to adding the blended dry ingredients. Once mixed, the compounded stocks have good scorch resistance and storage stability.
  • Composition: Terpolymer of vinylidene fluoride, hexafluoropropylene, and tetrafluoroethylene
  • Incorporated cure terpolymer gumstock
  • Process targets: compression and transfer molding, and calendering
  • Proprietary incorporated cure technology

Information provided by Dyneon, A 3M Company

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.86 g/cc1.86 g/cc
Mooney Viscosity 56
@Temperature 121 °C
56
@Temperature 250 °F
ML1+10
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 7575Press Cure 5 minutes @ 177°C, Post Cure 24 hours @ 260°C; ASTM D2240
Tensile Strength at Break 15.2 MPa2210 psiPress Cure 5 minutes @ 177°C, Post Cure 24 hours @ 260°C
Elongation at Break 310 %310 %Press Cure 5 minutes @ 177°C, Post Cure 24 hours @ 260°C
100% Modulus 3.72 MPa
@Strain 100 %
540 psi
@Strain 100 %
Press Cure 5 minutes @ 177°C, Post Cure 24 hours @ 260°C
Compression Set 36 %
@Temperature 200 °C,
Time 252000 sec
36 %
@Temperature 392 °F,
Time 70.0 hour
 
Thermal PropertiesMetricEnglishComments
Transformation Temperature -14.0 °C6.80 °FTR10; ASTM D1329
 
Component Elements PropertiesMetricEnglishComments
Fluorine, F 68.6 %68.6 %
 
Descriptive Properties
ColorOpaque Off-White
MH, Maximum Torque14.8 inch-lb100 cpm, 0.5° Arc, 6 Minutes @ 177°C
ML, Minimum Torque2.8 inch-lb100 cpm, 0.5° Arc, 6 Minutes @ 177°C
SolubilityKetones and Esters
t`50, Time to 50% cure1.2 minutes100 cpm, 0.5° Arc, 6 Minutes @ 177°C
t`90 - Time to 90% cure1.7 minutes100 cpm, 0.5° Arc, 6 Minutes @ 177°C
ts2 - Time to 2 in-lb rise from min0.9 minutes100 cpm, 0.5° Arc, 6 Minutes @ 177°C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Avient Dynaflex™ G7970-9001-02 Thermoplastic Elastomer (TPE)
Avient Dynaflex™ G7970-1001-00 Thermoplastic Elastomer (TPE)
ATG s.r.l. EPM Ethylene-Propylene Copolymer
ATG s.r.l. EPDM Ethylene-Propylene Terpolymer
AGC AFLAS® SZ TFE/P/VdF Fluoroelastomer

PDYNE144 / 34952

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.