MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Metal adhesives

(Viewing data as-entered. Click here to return)
Master Bond EP21AR Acid Resistant Two Component Epoxy
Categories: Polymer; Adhesive; Thermoset; Epoxy; Epoxy Adhesive

Material Notes: Key Features:
  • Cures at room temperature
  • Low viscosity
  • Outstanding chemical resistance to acids
  • High bond strength to similar and dissimilar substrates
  • Superb electrical insulation properties
  • For bonding, sealing, coating and encapsulating
Product Description: Master Bond EP21AR is a two component epoxy resin system for high performance bonding, sealing, coating and encapsulating. It has a convenient 100 to 50 mix ratio by weight and is formulated to cure at ambient temperatures or more quickly at elevated temperatures. It has exceptional resistance to a wide array of chemicals, particularly to acids (a more detailed list appears below). It is especially noteworthy for its resistance to sulfuric and hydrochloric acids. EP21AR is 100% reactive and contains no solvents or diluents. It has very low linear shrinkage upon cure. Also, it has outstanding physical properties and electrical insulation values. EP21AR can be used as an adhesive, sealant, coating, potting or encapsulating material. EP21AR is especially useful for coating tanks and other vessels that may contain acids. It is serviceable over the wide temperature range of -60°F to +250°F. It adheres well to a wide variety of substrates including metals, glass, ceramics and many rubbers and plastics. The standard version of this system has a lower viscosity with good flow. A nondrip version called EP21ARND is also available. Part A is clear and Part B is amber clear. This epoxy compound is widely used in aerospace, electronic, electrical, chemical processing applications and in other applications where chemical resistance to acids is needed.

Product Advantages:

  • 100% reactive compound does not contain any solvents or diluents
  • Versatile cure schedules; ambient temperature cures or fast elevated temperature cures
  • High bond strength to both similar and dissimilar Substrates
  • Wide service temperature service capability from 60°F to +250°F
  • Good electrical insulator
  • Low viscosity; ideal for potting and encapsulation
  • Outstanding chemical resistance, especially to acids

Information provided by Master Bond Inc.

Vendors: Master Bond is a leading manufacturer of adhesives, sealants, coatings and potting compounds. Master Bond’s vast product line consists of over 3,000 epoxy, polyurethane, silicone, cyanoacrylate and latex adhesives that vary in viscosity, cure speed, strength, chemical resistance, electrical properties, etc. Our custom adhesives offer design flexibility and provide excellent bonding performance. Visit www.masterbond.com.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Viscosity 4000 - 6000 cPPart B
 10000 - 15000 cPPart A
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength >= 8000 psi
Adhesive Bond Strength 2400 psiTensile lap, Aluminum to Aluminum
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity >= 1.00e+14 ohm-cm
Dielectric Constant 3.8
@Frequency 60 Hz
Dielectric Strength 440 V/mil
@Thickness 3.17 mm
 
Thermal PropertiesOriginal ValueComments
CTE, linear 40.0 - 45.0 µm/m-°C
Maximum Service Temperature, Air 250 °F
Minimum Service Temperature, Air -60.0 °F
 
Processing PropertiesOriginal ValueComments
Shelf Life 12.0 Month
@Temperature <=23.9 °C
in original, unopened containers
 
Descriptive Properties
Chemical ResistanceAcetic Acid (50%)1-6 Months Adversely Affected—Softened, Weight Gain or Loss
 Butyl AcetateNo Failures Observed after 14 Months, Test Discontinued
 CellosolveNo Failures Observed after 14 Months, Test Discontinued
 Chromic Acid (30%)1-6 Months Adversely Affected—Softened, Weight Gain or Loss
 Distilled WaterNo Failures Observed after 14 Months, Test Discontinued
 EthanolNo Failures Observed after 14 Months, Test Discontinued
 Formic Acid1-6 Months Adversely Affected—Softened, Weight Gain or Loss
 Hydrochloric Acid (10%)No Failures Observed after 14 Months, Test Discontinued
 Hydrochloric Acid (20%)No Failures Observed after 14 Months, Test Discontinued
 Hydrofluoric Acid (Concentrated)1-6 Months Adversely Affected—Softened, Weight Gain or Loss
 Nitric Acid (10%)No Failures Observed after 14 Months, Test Discontinued
 Nitric Acid (15%)No Failures Observed after 14 Months, Test Discontinued
 Nitric Acid (Concentrated)1-6 Months Adversely Affected—Softened, Weight Gain or Loss
 Phosphoric (10%, 20%, 30%)No Failures Observed after 14 Months, Test Discontinued
 Potassium Hydroxide (50%)No Failures Observed after 14 Months, Test Discontinued
 Sulfuric Acid (10%)No Failures Observed after 14 Months, Test Discontinued
 Sulfuric Acid (30%)No Failures Observed after 14 Months, Test Discontinued
 Sulfuric Acid (70%)No Failures Observed after 14 Months, Test Discontinued
 Sulfuric Acid (96-98%)No Failures Observed after 14 Months, Test Discontinued
Mixing Ratio1:1 by weightParts A to B

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Master Bond EP21TP-2 Two Component Polysulfide Epoxy Adhesive and Sealant
Abatron AboSeal 8104-17 Acrylic-Latex Based Sealant and Caulk; High-Density
Abatron AboSeal 8104-8 Polysulfide, Thixotropic Sealant and Caulk
Abatron AboSeal 8104-18 Vinyl-Acrylic-Latex Based Sealant and Caulk
Abatron AboSeal 8104-16 Acrylic-Latex Based Sealant and Caulk

PMASTM819 / 185412

Metal adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.