MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Biomerics Quadrathane™ ARC 75A- B20 Aromatic Polycarbonate TPU
Categories: Polymer; Thermoplastic; Polyurethane, TP

Material Notes: Quadrathane™ ARC is a family of aromatic polycarbonate-based thermoplastic polyurethane. It offers superior biocompatibility, superior chemical resistance, and oxidative stability for use in long term body implantable applications. It is naturally clear, hemocompatable, and is USP Class VI and ISO-10993 compliant. Quadrathane™ ARC is used across a wide range of medical applications including chronic indwelling catheters, feeding catheters, pacemaker leads, coatings, orthopedics, and other applications where superior chemical resistance is required.

Characteristics: Superior biocompatibility, superior chemical resistance, superior oxidative stability, hemocompatable, toughness..

Applications: Extrusion, Injection Molding, Solution

Information provided by Biomerics

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.34 g/cc1.34 g/ccASTM D792
Linear Mold Shrinkage 0.0080 - 0.012 cm/cm0.0080 - 0.012 in/inASTM 955
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 7575ASTM D2240
Tensile Strength, Ultimate 310 MPa45000 psiASTM D412
Elongation, Ultimate 650 %650 %ASTM D412
100% Modulus 3.79 MPa
@Strain 100 %
550 psi
@Strain 100 %
ASTM D412
300% Modulus 7.58 MPa
@Strain 300 %
1100 psi
@Strain 300 %
ASTM D412
Flexural Modulus 0.00896 GPa1.30 ksiASTM D790
 
Processing PropertiesMetricEnglishComments
Rear Barrel Temperature 177 °C351 °FInjection
Front Barrel Temperature 191 °C376 °FInjection
Nozzle Temperature 196 °C385 °FInjection
Zone 1 154 °C309 °FExtrusion
Zone 2 166 °C331 °FExtrusion
Zone 3 177 °C351 °FExtrusion
Zone 4 182 °C360 °FExtrusion
Adapter Temperature 182 °C360 °FExtrusion
Die Temperature 182 - 193 °C360 - 379 °FExtrusion
Melt Temperature 196 °C385 °FInjection
Mold Temperature 10.0 - 27.0 °C50.0 - 80.6 °FInjection
Drying Temperature 57.0 °C
@Time >=14400 sec
135 °F
@Time >=4.00 hour
Dew Point -40.0 °C-40.0 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PBIOMC029 / 250905

Elmet Technologies

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.