MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

SABIC LEXAN 244R PC (Asia Pacific)  (Unverified Data**)
Categories: Polymer; Thermoplastic; Polycarbonate (PC)

Material Notes: LEXAN 244R resin grade is a medium viscosity multi purpose product with improved flame resistance and release properties. It is also FDA food contact compliant available in limited colors.

Information provided by SABIC Innovative Plastics for Asia Pacific.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.20 g/cc1.20 g/ccASTM D 792
Density 1.19 g/cc0.0430 lb/in³ASTM D 792
Water Absorption 0.15 %
@Time 86400 sec
0.15 %
@Time 24.0 hour
ASTM D 570
Water Absorption at Saturation  0.35 %
@Temperature 23.0 °C
0.35 %
@Temperature 73.4 °F
ASTM D 570
 0.58 %
@Temperature 100 °C
0.58 %
@Temperature 212 °F
ASTM D 570
Linear Mold Shrinkage, Flow 0.0050 - 0.0070 cm/cm
@Thickness 3.20 mm
0.0050 - 0.0070 in/in
@Thickness 0.126 in
SABIC Method
Melt Flow 10.5 g/10 min
@Load 1.20 kg,
Temperature 300 °C
10.5 g/10 min
@Load 2.65 lb,
Temperature 572 °F
ASTM D 1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell M 7070ASTM D 785
Hardness, Rockwell R 118118ASTM D 785
Tensile Strength at Break 68.0 MPa9860 psiType I, 50 mm/min; ASTM D 638
Tensile Strength, Yield 62.0 MPa8990 psiType I, 50 mm/min; ASTM D 638
Elongation at Break 130 %130 %Type I, 50 mm/min; ASTM D 638
Elongation at Yield 7.0 %7.0 %Type I, 50 mm/min; ASTM D 638
Flexural Yield Strength 96.0 MPa13900 psi1.3 mm/min, 50 mm span; ASTM D 790
Flexural Modulus 2.34 GPa339 ksi1.3 mm/min, 50 mm span; ASTM D 790
Izod Impact, Notched 8.01 J/cm
@Temperature 23.0 °C
15.0 ft-lb/in
@Temperature 73.4 °F
ASTM D 256
Izod Impact, Unnotched 32.04 J/cm
@Temperature 23.0 °C
60.02 ft-lb/in
@Temperature 73.4 °F
ASTM D 4812
Tensile Impact Strength 577 kJ/m²275 ft-lb/in²Type S; ASTM D 1822
Falling Dart Impact 169 J
@Temperature 23.0 °C
125 ft-lb
@Temperature 73.4 °F
ASTM D 3029
Taber Abrasion, mg/1000 Cycles 10
@Load 1.00 kg
10
@Load 2.20 lb
CS-17; ASTM D 1044
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity >= 1.00e+17 ohm-cm>= 1.00e+17 ohm-cmASTM D 257
Dielectric Constant  2.96
@Frequency 1e+6 Hz
2.96
@Frequency 1e+6 Hz
ASTM D 150
 3.17
@Frequency 50.0 - 60.0 Hz
3.17
@Frequency 50.0 - 60.0 Hz
ASTM D 150
Dielectric Strength 14.9 kV/mm
@Thickness 3.20 mm
378 kV/in
@Thickness 0.126 in
in air; ASTM D 149
Dissipation Factor  0.00090
@Frequency 50.0 - 60.0 Hz
0.00090
@Frequency 50.0 - 60.0 Hz
ASTM D 150
 0.010
@Frequency 1e+6 Hz
0.010
@Frequency 1e+6 Hz
ASTM D 150
Comparative Tracking Index 250 - 400 V250 - 400 VPLC 2; UL 746A
Hot Wire Ignition, HWI 30 - 60 sec30 - 60 secPLC 2; UL 746A
High Amp Arc Ignition, HAI 60 - 120 arcs60 - 120 arcsPLC 1; UL 746A
High Voltage Arc-Tracking Rate, HVTR 25.4 - 80.0 mm/min1.00 - 3.15 in/minPLC 2; UL 746A
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 68.4 µm/m-°C
@Temperature -40.0 - 95.0 °C
38.0 µin/in-°F
@Temperature -40.0 - 203 °F
ASTM E 831
Specific Heat Capacity 1.25 J/g-°C0.299 BTU/lb-°FASTM C 351
Thermal Conductivity 0.270 W/m-K1.87 BTU-in/hr-ft²-°FASTM C 177
Deflection Temperature at 0.46 MPa (66 psi) 137 °C
@Thickness 6.40 mm
279 °F
@Thickness 0.252 in
unannealed; ASTM D 648
Deflection Temperature at 1.8 MPa (264 psi) 132 °C
@Thickness 6.40 mm
270 °F
@Thickness 0.252 in
unannealed; ASTM D 648
Vicat Softening Point 154 °C309 °FRate B/50; ASTM D 1525
UL RTI, Electrical 130 °C266 °FUL 746B
UL RTI, Mechanical with Impact 130 °C266 °FUL 746B
UL RTI, Mechanical without Impact 130 °C266 °FUL 746B
Flammability, UL94  V-2
@Thickness 1.47 mm
V-2
@Thickness 0.0579 in
UL 94
 V-0
@Thickness 5.99 mm
V-0
@Thickness 0.236 in
UL 94
Oxygen Index 25 %25 %ASTM D 2863
 
Optical PropertiesMetricEnglishComments
Refractive Index 1.5861.586ASTM D 542
Haze 1.0 %
@Thickness 2.54 mm
1.0 %
@Thickness 0.100 in
ASTM D 1003
Transmission, Visible 88 %88 %ASTM D 1003

**
This data sheet is not an active part of MatWeb and the information on it should not be considered reliable.
Inactive data sheets have usually been replaced with newer information on the same material. If this is the case, you can find the active data sheet by using any of our search tools, including the Quick Search box in the upper part of this page.
If you are unable to locate an active data sheet for this material, then this material is likely discontinued, although various other reasons may be behind its removal. In any event, do not rely on the information on this page to be accurate or maintained.
You may have reached this data sheet through an outdated bookmark or link. Please update your bookmark accordingly. We apologize if you have accessed this page through MatWeb’s usual search tools.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Chi Mei Polylac® PA-758 ABS - Transparent

PSABI47709 / 188784

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.