MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Metal adhesives

(Viewing data as-entered. Click here to return)
3M Pronto™ CA-5 Instant Adhesive
Categories: Polymer; Adhesive; Thermoset

Material Notes: One-part, room-temperature curing adhesive that is ready-to-use without metering or mixing. Bonded parts reach handling strength in 5-10 seconds on many applications.

A high viscosity, slower setting version of CA-4 Adhesive. Better adapted for filling gaps and uneven surfaces. Meets MIL-A-46050C Type II, Class 3.

Base is ethyl. It takes assembled parts 20-70 seconds to reach a strength where further handling and processing can take place. Times will depend on surface to be bonded, temperature and humidity. Average T-Peel at 75°F (24°C) is 1-2 PIW. Tested per ASTM D 1876-61T.

Information provided by 3M Adhesives Division.

Key Words: 3M Adhesives Division
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Viscosity 2000 - 3000 cP
 
Mechanical PropertiesOriginal ValueComments
Adhesive Bond Strength 6.20 MPa
@Temperature 23.9 °C
on ABS; ASTM D1002-64
 6.89 MPa
@Temperature 23.9 °C
on rigid PVC; ASTM D1002-64
 7.60 MPa
@Temperature 23.9 °C
on aluminum; ASTM D1002-64
 13.8 MPa
@Temperature 23.9 °C
on steel; ASTM D1002-64
 35.0 psi
@Temperature 23.9 °C
on nitrile rubber; ASTM D1002-64
 55.0 psi
@Temperature 23.9 °C
on neoprene rubber; ASTM D1002-64
 
Processing PropertiesOriginal ValueComments
Processing Temperature 20.0 °C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PMMB30 / 53477

Metal adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.