MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

SunChemical Gwent C2090324D8 Silver polymer paste
Categories: Other Engineering Material; Ceramic/Metallic Coating

Material Notes: This product is a thermoplastic screen printing ink, developed for use in membrane touch switch Applications as well as counter electrode in electrochemical sensors and conductive tracks. It may be screen printed on to flexible polymeric substrates, such as Polyimide, PEN and PET substrates, to create a highly conductive track for general circuitry. The ink has under gone electrical and mechanical testing which has shown that it is flexible.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Solids Content 64.5 - 65.5 %64.5 - 65.5 %
Viscosity 22000 - 27000 cP22000 - 27000 cP
Thickness 10.0 - 25.0 microns0.394 - 0.984 mil
 
Electrical PropertiesMetricEnglishComments
Surface Resistivity per Square 0.025 - 0.077 ohm0.025 - 0.077 ohm
 
Processing PropertiesMetricEnglishComments
Cure Time 10.0 - 30.0 min0.167 - 0.500 hour
 
Descriptive Properties
Conductive Filler TypeSilver (Ag)
Material TypeReady-To-Use Formulation
Recommended SubstratesPolyester, PVC, Polycarbonate or ceramic
Solvent SystemEthoxy Propanol or Sericol

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PFLEXCM90 / 179492

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.